Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group 3535 Epoxy Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group 5563 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group 6552 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group EN 5007 Epoxy Molding Compound Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group EPOXIDUR® 3580 EP Epoxy Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | IEC 60093 |
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures, excel.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+15 ohm | 1.00e+13 - 1.00e+15 ohm | Average value: 1.70e+14 ohm Grade Count:11 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | Average value: 6.79e+14 ohm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Surface Resistance | 12.0 - 1.00e+15 ohm | 12.0 - 1.00e+15 ohm | Average value: 8.00e+14 ohm Grade Count:15 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Surface Resistance | 1.10e+11 - 1.00e+15 ohm | 1.10e+11 - 1.00e+15 ohm | Average value: 1.44e+14 ohm Grade Count:8 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Surface Resistance | 1.00e+14 - 1.00e+15 ohm | 1.00e+14 - 1.00e+15 ohm | Average value: 6.00e+14 ohm Grade Count:9 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Surface Resistance | 10000 - 1.00e+15 ohm | 10000 - 1.00e+15 ohm | Average value: 2.50e+14 ohm Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+15 ohm | 1.00e+10 - 1.00e+15 ohm | Average value: 2.41e+14 ohm Grade Count:12 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Surface Resistance | 1.00e+10 - 1.00e+15 ohm | 1.00e+10 - 1.00e+15 ohm | Average value: 1.67e+14 ohm Grade Count:6 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+15 ohm | 1.00e+10 - 1.00e+15 ohm | Average value: 4.88e+13 ohm Grade Count:23 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+15 ohm | 1.00e+10 - 1.00e+15 ohm | Average value: 1.59e+14 ohm Grade Count:24 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Surface Resistance | 1.00e+6 - 1.00e+15 ohm | 1.00e+6 - 1.00e+15 ohm | Average value: 4.05e+13 ohm Grade Count:30 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+15 ohm | 1.00e+13 - 1.00e+15 ohm | Average value: 1.08e+14 ohm Grade Count:11 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Surface Resistance | 1.00e+10 - 1.00e+15 ohm | 1.00e+10 - 1.00e+15 ohm | Average value: 1.06e+14 ohm Grade Count:11 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+15 ohm | 1.00e+13 - 1.00e+15 ohm | Average value: 4.06e+14 ohm Grade Count:9 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Surface Resistance | 1.00e+11 - 1.00e+15 ohm | 1.00e+11 - 1.00e+15 ohm | Average value: 3.55e+14 ohm Grade Count:20 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Surface Resistance | 1000 - 1.00e+15 ohm | 1000 - 1.00e+15 ohm | Average value: 1.54e+14 ohm Grade Count:15 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Surface Resistance | 1.00e+13 - 1.00e+15 ohm | 1.00e+13 - 1.00e+15 ohm | Average value: 2.57e+14 ohm Grade Count:12 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Surface Resistance | 1.30e+13 - 1.00e+15 ohm | 1.30e+13 - 1.00e+15 ohm | Average value: 8.03e+14 ohm Grade Count:5 |
Overview of materials for Nylon, Flexible Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Flexible Alloy". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Surface Resistance | 1.00e+10 - 1.00e+15 ohm | 1.00e+10 - 1.00e+15 ohm | Average value: 5.25e+14 ohm Grade Count:4 |
Overview of materials for Polycarbonate, 40% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 40% Glass Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+15 ohm | 1.00e+13 - 1.00e+15 ohm | Average value: 2.62e+14 ohm Grade Count:5 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Surface Resistance | 1.00e+13 - 1.00e+15 ohm | 1.00e+13 - 1.00e+15 ohm | Average value: 1.90e+14 ohm Grade Count:9 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Surface Resistance | 10000 - 1.00e+15 ohm | 10000 - 1.00e+15 ohm | Average value: 1.67e+14 ohm Grade Count:6 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Surface Resistance | 3000 - 1.00e+15 ohm | 3000 - 1.00e+15 ohm | Average value: 1.35e+14 ohm Grade Count:23 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Surface Resistance | 0.100 - 1.00e+15 ohm | 0.100 - 1.00e+15 ohm | Average value: 1.08e+14 ohm Grade Count:23 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |