Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 465E2R30012 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 513E3720008 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Acetate 105E1R26033 Clear, Trsp Cellulose Acetate Plasticizer 29%. Weight loss on heating = 2.6% per ASTM D 707. Soluble matter loss = 0.4% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Acetate 105E2R30025 Natural, Trsp Cellulose Acetate Plasticizer 33%. Weight loss on heating = 3.6% per ASTM D 707. Soluble matter loss = 0.6% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 264A3720013 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 13%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 264E4861310 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE Butyrate 264E0096908 Natural, Trsp TENITE cellulosic plastic.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 285A2R30023 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 285A3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 485A2R30016 Natural Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.TENITE cellulosic plastics are noted for their excellent balance of properties - toughness,.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 485A2R30023 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 530A3720016 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 530E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 550E4861316 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 575E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 576E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 307A2R30018 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 350E0096912 Natural, Trsp Cellulose Acetate Propionate Plasticizer 13%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 360E0096916 Natural, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 371A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 371A2R30012 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 383A2R30007 Natural, Trsp Cellulose Acetate Propionate Plasticizer 7%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 383A2R30009 Natural, Trsp Cellulose Acetate Propionate Plasticizer 9%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
CTE, linear | 15.0 - 17.0 µm/m-°C @Temperature 1000 °C |
8.33 - 9.44 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CSN-309NM,Insert Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 358A4000008 Clear, Trsp Cellulose Acetate Propionate Plasticizer 14%. Weight loss on heating = 0.6% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 16.0 - 17.0 µm/m-°C | 8.89 - 9.44 µin/in-°F | IPC TM-650 2.4.41 |
Arlon 33N Polyimide Laminate and Prepreg High reliability and high temperature material33N is a flame retardant polyimide laminate and prepreg system where the excellent high performance properties of polyimide need to be combined with fla.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 465A3720010 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 10%. Weight loss on heating = 0.9% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 17.0 - 17.0 µm/m-°C @Temperature 140 - 180 °C |
9.44 - 9.44 µin/in-°F @Temperature 284 - 356 °F |
Average value: 17.0 µm/m-°C Grade Count:1 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 350E0096914 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 465E3720008 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 581A3720016 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |