Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm @Thickness 3.20 mm |
0.00300 - 0.00500 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 301 FR UV Polycarbonate (PC), Glass Fiber - Flame Retardant - Non-PBBO/E The RTP series of flame retardant, glass fiber reinforced polycarbonate materials offer dimensional stability with improved heat distortion and ignition resistance performance over the base resin. .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00325 cm/cm Grade Count:12 |
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.00500 cm/cm | 0.000500 - 0.00500 in/in | Average value: 0.00215 cm/cm Grade Count:15 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Linear Mold Shrinkage | 0.000 - 0.00500 cm/cm | 0.000 - 0.00500 in/in | Average value: 0.00133 cm/cm Grade Count:40 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00269 cm/cm Grade Count:8 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00309 cm/cm Grade Count:11 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00500 cm/cm | 0.00100 - 0.00500 in/in | Average value: 0.00288 cm/cm Grade Count:3 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm @Thickness 3.20 mm |
0.00300 - 0.00500 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 2501 FR Polycarbonate/ABS Alloy (PC/ABS), Glass Fiber - Flame Retardant - Non-PBBO/E - UL94 V-0 |
|||
Linear Mold Shrinkage | 0.00200 - 0.00500 cm/cm @Thickness 3.20 mm |
0.00200 - 0.00500 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 205 TFE 10 Z Nylon 6/6 (PA) Glass Fiber - PTFE Lubricated - FDA Compliant Ingredients |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU650N ABS Heat Resistant Medium/High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU650NH ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU650N ABS Heat Resistant Medium/High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron TG3MM ABS Injection Molding Grade Medium Flow, Medium Impact, high RigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2007LF SAN Resin High Rigidity Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron HR60N ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IM14GM ABS Injection Molding Grade High Rigidity, Medium Impact, Good paintabilityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU670 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2000 Glitter SAN Resin High Transparent SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS1000 SAN Resin Clear SANInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Santron IMS1000M SAN Resin Clear SAN, Pen barrel applicationInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU600N ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00300 - 0.00500 cm/cm | 0.00300 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron KU602 ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00500 - 0.00500 cm/cm @Temperature 80.0 - 80.0 °C |
0.00500 - 0.00500 in/in @Temperature 176 - 176 °F |
Average value: 0.00500 cm/cm Grade Count:1 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00500 cm/cm | 0.00400 - 0.00500 in/in | ASTM D955 |
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali |