Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 0.345 - 80.0 MPa | 50.0 - 11600 psi | Average value: 7.65 MPa Grade Count:872 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Tensile Strength, Ultimate | 25.0 - 80.0 MPa @Temperature 60.0 - 150 °C |
3630 - 11600 psi @Temperature 140 - 302 °F |
Average value: 55.0 MPa Grade Count:2 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Tensile Strength, Ultimate | 0.345 - 80.0 MPa | 50.0 - 11600 psi | Average value: 11.6 MPa Grade Count:42 |
Overview of materials for Styrenic TPE
(Unverified Data**) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe.. |
|||
Tensile Strength, Ultimate | 55.2 - 80.0 MPa | 8000 - 11600 psi | Average value: 66.9 MPa Grade Count:79 |
Overview of materials for Polycarbonate, UV Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a.. |
|||
Tensile Strength, Ultimate | 50.0 - 80.0 MPa @Temperature 60.0 - 120 °C |
7250 - 11600 psi @Temperature 140 - 248 °F |
Average value: 66.7 MPa Grade Count:1 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Tensile Strength, Ultimate | 44.1 - 80.0 MPa | 6400 - 11600 psi | Average value: 67.0 MPa Grade Count:14 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Tensile Strength, Ultimate | 8.48 - 80.0 MPa | 1230 - 11600 psi | Average value: 16.6 MPa Grade Count:51 |
Overview of materials for PVC, Uncompounded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Uncompounded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Tensile Strength, Ultimate | 9.00 - 80.0 MPa | 1310 - 11600 psi | Average value: 30.1 MPa Grade Count:177 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Ultimate | 68.7 - 80.0 MPa | 9970 - 11600 psi | Average value: 75.3 MPa Grade Count:3 |
Overview of materials for Phenolic, Graphite Cloth Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Graphite Cloth Composite". Each property range of values reported is minimum and maximum value.. |
|||
Tensile Strength, Ultimate | 70.0 - 80.0 MPa @Temperature 130 - 175 °C |
10200 - 11600 psi @Temperature 266 - 347 °F |
Average value: 66.6 MPa Grade Count:2 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Tensile Strength, Ultimate | 70.0 - 80.0 MPa @Time 1.80e+7 - 7.20e+7 sec |
10200 - 11600 psi @Time 5000 - 20000 hour |
Average value: 66.6 MPa Grade Count:2 |
Overview of materials for Nylon 66, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Tensile Strength, Ultimate | 22.0 - 80.0 MPa @Temperature 80.0 - 120 °C |
3190 - 11600 psi @Temperature 176 - 248 °F |
Average value: 50.9 MPa Grade Count:1 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Ultimate | 22.0 - 80.0 MPa @Strain 1.00 - 8.00 % |
3190 - 11600 psi @Strain 1.00 - 8.00 % |
Average value: 50.9 MPa Grade Count:1 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Ultimate | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Alliance BIF-11 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Alliance BIF-17 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Alliance BIF-19 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Alliance BIF-2 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 30.0 - 80.0 MPa | 4350 - 11600 psi | |
Alliance BIF-16 Bonded (Composite) Magnetic Material |
|||
Tensile Strength, Ultimate | 42.0 - 80.0 MPa | 6090 - 11600 psi | Average value: 71.4 MPa Grade Count:12 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Tensile Strength, Ultimate | 23.0 - 80.0 MPa @Temperature 160 - 160 °C |
3340 - 11600 psi @Temperature 320 - 320 °F |
Average value: 68.8 MPa Grade Count:2 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Ultimate | 23.0 - 80.0 MPa @Strain 0.600 - 3.00 % |
3340 - 11600 psi @Strain 0.600 - 3.00 % |
Average value: 68.8 MPa Grade Count:2 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Ultimate | 50.0 - 80.0 MPa @Temperature 160 - 160 °C |
7250 - 11600 psi @Temperature 320 - 320 °F |
Average value: 70.2 MPa Grade Count:1 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Tensile Strength, Ultimate | 50.0 - 80.0 MPa @Strain 0.600 - 1.40 % |
7250 - 11600 psi @Strain 0.600 - 1.40 % |
Average value: 70.2 MPa Grade Count:1 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Tensile Strength, Ultimate | 40.0 - 80.0 MPa @Temperature 60.0 - 120 °C |
5800 - 11600 psi @Temperature 140 - 248 °F |
Average value: 60.0 MPa Grade Count:2 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Tensile Strength, Ultimate | 0.800 - 80.0 MPa | 116 - 11600 psi | Average value: 29.0 MPa Grade Count:318 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Tensile Strength, Ultimate | 29.0 - 80.0 MPa @Temperature -40.0 - 120 °C |
4210 - 11600 psi @Temperature -40.0 - 248 °F |
Average value: 45.0 MPa Grade Count:4 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Tensile Strength, Ultimate | 9.00 - 80.0 MPa @Temperature 60.0 - 120 °C |
1310 - 11600 psi @Temperature 140 - 248 °F |
Average value: 31.0 MPa Grade Count:2 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |