Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.640 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ NT-818.G002-8000 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256 |
Network Polymers NPP 25-0202 C Description: Copolymer Polypropylene, Clarified RandomInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256 |
Polymer Resources AH-GP3-[color]-H Acetal Homopolymer, High Flow Resin, Heat Stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.20 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® SF-20CF/000 Polyphenylene Sulfide (PPS)
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256A |
LyondellBasell Astryn 73F5-1 Polypropylene Copolymer, 10% Calcium Carbonate Key Features: medium high melt flow, medium modulus, mineral-filled polypropylene copolymer, excellent impact and stiffness balance, good colorability, good aesthetics, very good processabilityAppli.. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY RX05497 PA 66 LNP LUBRILOY* RX05497 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DD0009E PC (Asia Pacific) LNP* Stat-kon* DD0009E is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Electrafil® DB-1200/SS/4 ABS, 4% Stainless Steel Fiber Reinforced (dry blend) Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL.. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific) LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P.. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF20 HS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp AF002L ABS (Asia Pacific) LNP* Thermocomp* AF002L is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Low Extractible.This data was supplied by SABIC.. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Statiblend® ABS GF15 AS 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Statiblend® POM CO AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeature: Antistatic and ConductiveTPCI# 60000114Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.640 J/cm @Temperature 23.0 °C |
1.20 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp AF002L ABS LNP* Thermocomp* AF002L is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Low Extractible.This data was supplied by SABIC.. |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256 |
A. Schulman PP 1116-01 Polypropylene Molding Grade Copolymer Polypropylene DescriptionPolypropylene PP 1116-01 is a molding grade copolymer polypropylene with improved low temperature toughness and good room temperature toughness. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | |
Toyobo ECOVYLOPET® EMC2310 PET Bottle Recycling Grade, 10% Glass Reinforced Features: PET Bottle Recycling Grade, 10% Glass Fiber Reinforced, General PurposeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.. |
|||
Izod Impact, Notched | 0.640 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PPC-CC10 Natural Copolymer Polypropylene, 10% Calcium Carbonate Filled Information provided by Entec |
|||
Izod Impact, Notched | 0.641 J/cm @Temperature 22.8 °C |
1.20 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant PBTSP0008WT-199 Polybutylene Terephthalate, Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.641 J/cm | 1.20 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P-05FG-0870 5% Glass Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | >= 0.641 J/cm | >= 1.20 ft-lb/in | ASTM D256 |
Buckeye Polymers BP RPP 3009 GKW Polypropylene, Glass Filled Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en.. |
|||
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® PA6/6 GF20 FR 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman. |