Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | |
Murtfeldt Murlubric® [FS] Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Thermal Conductivity | 0.231 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NH9294 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics EXTEM UH1026 TPI Blend High heat amorphous TPI Blend, Chemical Resistant, High Flow, IR-Transparent |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | |
Dow Isoplast® 302 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 302 resin is a clear amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include clarity, excellent chemical resistance, toughness and high he.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1-1120 Polyamide 66, with PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1t-7503 Polyamide 6/6T, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon TFM Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® NSB 90 BK Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 22007-4 |
GEHR Plastics PA 6 C Nylon 6 Cast Very stressed-relieved and high-molecular weight PA6.Temperature resistant from -40° to approx. 100°C and high stiffness, hardness and toughness. The good mechanical characteristics will be ac.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1/TF/18/SI/2 Polyamide 66, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL SE1 PPE+HIPS (Europe-Africa-Middle East) NORYL SE1 is an unfilled, flame retardant material with a Vicat B/120 of 140°C according ISO 306. NORYL SE1 is V1 at 1.47 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM AUT195 PEI+PCE High flow Polyetherimide blend for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of 195C (SABIC test method). |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® XE5515BL Polyphenylene Sulfide Alloy (PPS Alloy), 15% Glass Fiber Ryton® XE5515BL 15% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength and chemical resistance at elevated temperatures and is suitable for extrusi.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER (Asia Pacific) PC+Polyester, UV Stabilized, Transparent |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Asia Pacific) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Noryl HIN120P PPE+HIPS (Europe-Africa-Middle East) Noryl HIN120P is designed for selected one layer water-based paint systems. Noryl HIN120P has a Vicat B/120 of 120 °C and is targetedThis data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Noryl EN110 PPE+HIPS (Europe-Africa-Middle East) NORYL EN110 is an extrusion material with a Vicat B/120 of 115°C according ISO 306. NORYL EN110 is a standard extrusion grade for applications where medium temperature resistance is required.This.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL ENV105 PPE+HIPS (Europe-Africa-Middle East) NORYL ENV105 is an impact modified extrusion grade with a Vicat B/120 of 115C according ISO 306. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 1200 G Zellamid® 1200 G is manufactured by an activated anionic reaction. Finished and semi-finished parts are produced by a static cast process. This process makes it possible to produce a material wit.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | |
Hippe PA 66 Nylon 66 The polyamide with high degree of hardness, stiffness, scuff strength and stability of shape under heat. Preferred polyamide for components subjected to high load and heat stress in electrical, mec.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 125 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 257 °F |
|
Dow SiLK™ I 550 Semiconductor Dielectric Resin SiLK™ I 550 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 550 is compatible with.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 125 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 257 °F |
|
Dow SiLK™ I300 380 Semiconductor Dielectric Resin SiLK™ I300 380 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 380 is compatibl.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 125 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 257 °F |
|
Dow SiLK™ I300 560 Semiconductor Dielectric Resin SiLK™ I300 560 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 560 is compatibl.. |
|||
Thermal Conductivity | 0.230 - 0.250 W/m-K | 1.60 - 1.74 BTU-in/hr-ft²-°F | Average value: 0.244 W/m-K Grade Count:15 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |