Mechanical Properties Metric English Comments
Izod Impact, Notched 0.641 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products G20P100-00 20% Glass Fiber Reinforced Polypropylene, Natural
Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.641 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
ASTM D256
RheTech Products G20P100-01 20% Glass Fiber Reinforced Polypropylene, Black
Applications: Arm rest insertVacuum canisterStorage binConsolesBattery traysInjection molding conditions reported in table.Information provided by RheTech Products.
Izod Impact, Notched 0.641 J/cm

@Temperature 22.8 °C
1.20 ft-lb/in

@Temperature 73.0 °F
ASTM D256
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled  (discontinued **)
Information provided by MRC Polymers Inc.
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 4300 S-1010 Polysulfone/Polycarbonate Alloy (PSU/PC), Glass Fiber - UL94
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 800 TFE 15 Acetal (POM), PTFE Lubricated
Izod Impact, Notched 0.641 J/cm

@Thickness 3.20 mm
1.20 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company RTP 900 TFE 10 Z Polysulfone (PSU); PTFE Lubricated - FDA Compliant Ingredients
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 901 Polysulfone (PSU), Glass Fiber
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Fiberfil® J-60/20/H Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Lucent Polymers GPP-140 Polypropylene Homopolymer, 40% Glass Fiber Reinforced, Chemically Coupled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES Luriblend® PSU GF20 TL5 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill FR® PA4/6 GF15 FR HS L 15% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat St..
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
Westlake Plastics Propylux® Void-Free Polypropylene
Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance to abrasion. These properties make it suitable fo..
Izod Impact, Notched 0.641 J/cm

@Thickness 3.20 mm
1.20 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company RTP 1302 P-1 Polyphenylene Sulfide (PPS); Glass Fiber
Izod Impact, Notched 0.641 J/cm

@Thickness 3.20 mm
1.20 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company RTP 2185 Polyetherimide (PEI); Carbon Fiber
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
A. Schulman SCHULAMID® 66 GF15H 15% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
Izod Impact, Notched 0.641 J/cm

@Thickness 3.20 mm
1.20 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company EMI 333 G FR Polycarbonate (PC); 20% Glass Fiber - 15% Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - Flame Retardant
Izod Impact, Notched 0.641 J/cm

@Temperature 22.8 °C
1.20 ft-lb/in

@Temperature 73.0 °F
ASTM D256
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK)
TECAPEEK™ high performance polymer has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties al..
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
Diamond Polymers DIAMALOY 1001 CF20 20% Carbon Fiber Filled ABS
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256A
Dow C700-35N Polypropylene Impact Copolymer Resin
OverviewGood mold fillabilityHigh stiffnessFast set-upContains a nucleating additiveComplies with: U.S. FDA FCN 843, Canadian HPFB No ObjectionDOW C700-35N Polypropylene Resin is intended for use in..
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
Ensinger Tecast Vekton™ 6PAG Graphite-Filled Cast Nylon 6 (PA6)
Tecast® 6PAG is a graphite powder-filled with properties similar to MoS2-filled but better suited to wet applications.General Tecast® Cast Nylon Information: Tecast cast nylon, available in a vari..
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334G30CL Glass Reinforced Coupled
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
ASTM D256
WR90Z POM, UV Resistant
« WR90Z is a standard nominal 9 melt flow rate based acetal copolymer stabilized to provide maximum ultraviolet radiation resistance in outdoor applications while retaining a good balance of proper..
Izod Impact, Notched 0.641 J/cm

@Thickness 3.20 mm
1.20 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company RTP 899 X 130047 A Acetal (POM); Static Dissipative - Impact Modified - PTFE Lubricated  (disconti
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Izod Impact, Notched 0.641 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
PolyOne Stat-Tech™ ES-06CF-09GF/000 Polyethersulfone, Glass/Carbon Fiber Filled  (discontinued **)
Description/Features:Glass/Carbon Fiber ReinforcedInformation provided by PolyOne Corporation.
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D 256
RTP Company RTP 299 A X 92682 A Nylon 6 (PA), High Gravity Compound - Easy Molding
Izod Impact, Notched 0.641 J/cm

@Thickness 3.20 mm
1.20 ft-lb/in

@Thickness 0.126 in
ASTM D 256
RTP Company RTP 4799 X 117571 E Polytrimethylene Terephthalate (PTT) Glass Fiber - Flame Retardant - Halogen Free
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
D 256
RTP Company RTP 801 TFE 10 DEL Acetal (POM), Glass Fiber Reinforced - PTFE Lubricated
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D 256
RTP Company RTP 882 Acetal (POM), Carbon Fiber
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm
1.20 ft-lb/in

@Thickness 0.125 in
ASTM D256
RTP Company RTP 4705 FR NH  Polytrimethylene Terephthalate (PTT) Glass Fiber 30% - Non Halogen Flame Retardant
Glass Fiber 30% - Non Halogen Flame RetardantComments:Glass FiberFlame RetardantHalogen FreeUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect..