Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.74 J/cm - NB | 7.00 ft-lb/in - NB | Average value: 5.76 J/cm Grade Count:17 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP AF004XXY ABS LNP* Thermocomp* AF004XXY is a compound based on ABS containing 20% glass fiber. |
|||
Izod Impact, Unnotched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D4812 |
A. Schulman ComAlloy® E-12421 Reinforced High Flow Polyamide Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 3.74 J/cm | 7.00 ft-lb/in | ASTM D4812 |
A. Schulman SCHULADUR® B GF15 15% Glass Fiber Reinforced PET Information provided by A. Schulman. |
|||
Izod Impact, Unnotched | 3.74 J/cm | 7.01 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 754 Glass Reinforced, Flow Enhanced, PPS Alloy, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 3.74 - 5340 J/cm | 7.00 - 10000 ft-lb/in | Average value: 7.43 J/cm Grade Count:9 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Izod Impact, Unnotched | 3.74 - 11.2 J/cm | 7.00 - 21.0 ft-lb/in | Average value: 5.94 J/cm Grade Count:8 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Izod Impact, Unnotched | 3.74 - 8.54 J/cm | 7.00 - 16.0 ft-lb/in | Average value: 6.53 J/cm Grade Count:10 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |