Polymer Property : Charpy Impact, Notched = 3.81 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Nilit FRIANYL A63 H-GV35 Nylon 6.6 for injection molding, 35% glass fiber reinforced
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HF500R PC (Europe-Africa-Middle East)
LEXAN HF500R is an easy flow, 9% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and impact performance.
Charpy Impact, Notched 0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
Covestro Apec® DP 1-9359/5 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba..
Charpy Impact, Notched 0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 179 eA
Lehmann & Voss LUVOCOM® 1105-8417 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
LATI Lasulf G/20 PSU, 20% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific)
VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings.
Charpy Impact, Notched 0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 179/2C
SABIC Innovative Plastics Valox® 4521 PBT (Europe-Africa-Middle East)
VALOX 4521 is a high flow, 19.5% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications.
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Valox® SHF436HR PBT (Asia Pacific)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific)
PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179
Teijin Panlite® G-3310M Isotropic, Glass Fiber Reinforced Polycarbonate Resin
Reinforced with 10 % of special GF and least anisotropy grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need good appearance and mechanical propertyPrecisio..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Total Polystyrene Impact 3450 Aesthetic, High Fluidity, High Heat Resistance, High Impact Polystyrene
POLYSTYRENE IMPACT 3450 is a high impact polystyrene with high heat resistance, good flow, high stiffness and good aesthetics. With such an ideal balance of properties, POLYSTYRENE IMPACT 3450 is w..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eU
Total PSI 4440(EU) High Impact Polystyrene
4440 is a high impact polystyrene for the injection molding of parts demanding good dimensional stability at high temperatures, particularly front and back covers for television sets. In addition, ..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Borealis Borpact™ SE920MO Polypropylene Homopolymer for Injection Molding
Borpact SE920MO is a high impact and transparent polypropylene. Borpact SE920MO is a new generation polypropylene having properties that were earlier not possible to combine. Borpact SE920MO offers..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179
Total PPR 6280 Random Copolymer Polypropylene, Cast Film Extrusion Grade
Total Petrochemicals PPR 6280 is a random copolymer polypropylene with a melt flow index of 7 g/10 min suitable for the cast extrusion of films with outstanding optical properties and easy heat weld..
Charpy Impact, Notched 0.800 J/cm²

@Temperature 30.0 °C
3.81 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® EBV-15H black 9697 PA6-GF15
Product description: Grilon EBV-15H black 9697 is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 15% glass fibers. Grilon EBV-15H black 9697 has the following important prop..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
dry; ISO 179/1eA
EMS-Grivory Grivory® GTR 45 PA6I/6T
Product description: Grivory GTR 45 is a transparent engineering thermoplastic based on amorphous, partially aromatic copolyamide for injection molding. Compared to other semi crystalline polyamides..
Charpy Impact, Notched 0.800 J/cm²

@Temperature 30.0 °C
3.81 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® HTV-4H1 nat PA6T/6I-GF40
Product description: Grivory HTV-4H1 natural is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac..
Charpy Impact, Notched 0.800 J/cm²

@Temperature 30.0 °C
3.81 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
EMS-Grivory Grivory® TSG-35/4 PA666-GF35
Product description: Grilon TSG-35/4 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers. Grilon TSG-35/4 has the following important properties: Good flo..
Charpy Impact, Notched 0.800 J/cm²

@Temperature 30.0 °C
3.81 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
EMS-Grivory Grivory® TSG-35/4 W black 9832 PA666-GF35
Product description: Grilon TSG-35/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 35% glass fibers, modified for parts with high thermal demands. Grilon TSG-..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
DuPont Performance Polymers Crastin® SK642FR NC010 Polybutylene Terephthalate (PBT)
15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK642FR is a 15% glass fibre reinforced flame retardant polybutylene terephthalate for injection moulding.It has a UL94 V-0 ra..
Charpy Impact, Notched 0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
DuPont Performance Polymers Delrin® 525GR NC000 Acetal (POM)  (Unverified Data**)
25% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 525GR NC000 is a 25% glass reinforced acetal homopolymer for injection molding. It has very high strength stiffness and high deflectio..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Celanese CELANEX 5200-2 PBT, 15% Glass Reinforced
Celanex 5200-2 is a 15% fiberglass reinforced polyester with improved surface finish. Celanex 5200-2 contains an internal lubricant.Information provided by Celanese
Charpy Impact, Notched 0.800 J/cm²

@Temperature 23.0 °C
3.81 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Conditioned, 10% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179
BASF Ultradur B 4406 G6 Q113 30% Glass Filled PBT
Ultradur B4406 G6 Q113 is an UL V0 injection molding, PBT grade with 30% glass fiber reinforcement.
Charpy Impact, Notched 0.800 J/cm²

@Temperature -30.0 °C
3.81 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Celanese Hostaform® SXT90Z-02 XAP POM, Impact Modified
Hostaform« acetal copolymer grade SXT90Z-02 XAP is UV stabilized, impact modified material available in a range of colors for automotive interior applications plus meets the typical low emission re..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO179
Beijing Chemical Industry KAIFA® HN201-G10 PA6 Resin
10% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group)
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/IeA
CENTROPLAST CENTROGUARD Polyoxymethylene, Antimicrobial
During the modification with POM CG, antimicrobial substances are included in the basic polyoxymethylene polymer, which provide an effective and long lasting solution against unwanted growth of micr..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179
Teijin Panlite® GV-3410R High Flame Retardancy, Glass Fiber Reinforced Polycarbonate Resin
GF 10% reinforced, improved flame retardance and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecis..
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Xenoy® X5630P PET+PC (Europe-Africa-Middle East)
Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications