Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Mold Temperature 135 - 149 °C
275 - 300 °F
PolyOne Edgetek® PF-05GF/000 FR MR Polysulfone (PSU)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1391 Polyphenylene Sulfide (PPS), Carbon Fiber  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Mold Temperature 135 - 163 °C
275 - 325 °F
LNP Lubricomp® PDX-O-90351 Polyphenylene Sulfide, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Mold Temperature 135 - 163 °C
275 - 325 °F
RTP Company RTP 4005 TFE 10 Polyphthalamide (PPA), Glass Fiber - PTFE Lubricated
Mold Temperature 135 - 163 °C
275 - 325 °F
RTP Company RTP 4085 SI 2 Polyphthalamide (PPA), Carbon Fiber - Silicone Lubricated
Mold Temperature 135 - 163 °C
275 - 325 °F
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2100 AR 10  Polyetherimide (PEI) Aramid Fiber 10%  (discontinued **)
Aramid Fiber 10%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2100 HF TFE 15  Polyetherimide (PEI) PTFE 15% - High Flow  (discontinued **)
PTFE 15% - High FlowComments:PTFE LubricatedHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company EMI 2180.5  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 5%  (dis
Shielding - Nickel-Coated Carbon Fiber 5%Comments:EMI/RFI ShieldingESD ProtectionNickel-Coated Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigm..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company EMI 2184  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 25%  (disc
Shielding - Nickel-Coated Carbon Fiber 25%Comments:EMI/RFI ShieldingESD ProtectionNickel-Coated Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pig..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company EMI 2185  Polyetherimide (PEI) Shielding - Nickel-Coated Carbon Fiber 30%  (disc
Shielding - Nickel-Coated Carbon Fiber 30%Comments:EMI/RFI ShieldingESD ProtectionNickel-Coated Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pig..
Mold Temperature 135 - 160 °C
275 - 320 °F
Lehmann & Voss LUVOCOM® 20-7638 Polyphthalamide, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Mold Temperature 135 °C
275 °F
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned)
Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th..
Mold Temperature 135 °C
275 °F
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned)
Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1305 TFE 13 SI 2 Polyphenylene Sulfide (PPS), Glass Fiber Reinforced - PTFE & Silicone Lubricated
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1305 TFE 20 Polyphenylene Sulfide (PPS), Glass Fiber Reinforced - PTFE Lubricated
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1378 Polyphenylene Sulfide (PPS), Glass Fiber - PTFE Lubricated
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1385 TFE 20 Polyphenylene Sulfide (PPS), Carbon Fiber Reinforced - PTFE Lubricated
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1400 AG-360 M1 Polyethersulfone (PES), Glass Fiber - UL94 V-1
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2183 Polyetherimide (PEI); Carbon Fiber
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2184 L Polyetherimide (PEI) Carbon Fiber - Easy Molding
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company ESD A 1307 Polyphenylene Sulfide (PPS), Glass Fiber - ESD Protection - Static Dissipative
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2199 X 120440 G Polyetherimide (PEI) Carbon Nanotube - ESD Protection - High Purity
Mold Temperature 135 - 149 °C
275 - 300 °F
Celanese CoolPoly® E5103 Thermally Conductive Polyphenylene Sulfide
CoolPoly E series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows ..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1405 L  Polyethersulfone (PES) Glass Fiber 30% - Lubricated  (discontinued *
Glass Fiber 30% - LubricatedComments:Glass FiberLubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided b..
Mold Temperature 135 - 149 °C
275 - 300 °F
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1401 Polyethersulfone (PES), Glass Fiber
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 1483 N Polyethersulfone (PES), Carbon Fiber - High Viscosity
Mold Temperature 135 - 177 °C
275 - 350 °F
RTP Company RTP 2103 TFE 10 Polyetherimide (PEI), Glass Fiber - PTFE Lubricated
Mold Temperature 135 °C
275 °F
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of ..