Albis Plastics EVA Masterbatch MB 50 Black  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate; Molded/Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics EVA Masterbatch MB 50 Black  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Black Polyolefin Color Concentrate; 48.0% pigmentCharacteristics: Low Density Polyethylene Base ResinProcessing: Formulated for injection moldingData supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
Base density
1.21 g/cc
0.0437 lb/in³
Concentrate