Polymer Property : Melt Temperature = 343 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 343 - 391 °C
649 - 736 °F
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boil..
Melt Temperature 343 - 385 °C
649 - 725 °F
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)  (Unverified Data**)
Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids...
Melt Temperature 343 - 391 °C
649 - 736 °F
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)  (Unverified Data**)
Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn..
Melt Temperature 343 - 382 °C
650 - 720 °F
Molding
PolyOne Edgetek® PF-05GF/000 Polysulfone, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 343 - 388 °C
649 - 730 °F
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled
Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h..
Melt Temperature 343 - 399 °C
649 - 750 °F
Solvay Specialty Polymers Udel® GF-130 Polysulfone (PSU), Glass Fiber
Udel® GF-130, resin is a 30% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical ..
Melt Temperature 343 - 399 °C
649 - 750 °F
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU), 30% Glass Fiber
Veradel® 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, ..
Melt Temperature 343 - 377 °C
650 - 710 °F
RTP Company RTP 1400 AG-330 Polyethersulfone (PES), Glass Fiber
Melt Temperature 343 - 377 °C
650 - 710 °F
RTP Company RTP 1400 AG-360 M1 Polyethersulfone (PES), Glass Fiber - UL94 V-1
Melt Temperature 343 - 377 °C
650 - 710 °F
RTP Company RTP 1402 N Polyethersulfone (PES), Glass Fiber - High Viscosity
Melt Temperature 343 - 377 °C
650 - 710 °F
RTP Company RTP 1407 N Polyethersulfone (PES), Glass Fiber - High Viscosity
Melt Temperature 343 - 377 °C
650 - 710 °F
RTP Company RTP 1407 TFE 15 Polyethersulfone (PES); Glass Fiber - PTFE Lubricated
Melt Temperature 343 - 377 °C
650 - 710 °F
RTP Company RTP 1482 N Polyethersulfone (PES), Carbon Fiber - High Viscosity
Melt Temperature 343 - 377 °C
650 - 710 °F
RTP Company RTP 1482 N TFE 15 Polyethersulfone (PES), Carbon Fiber - PTFE Lubricated
Melt Temperature 343 - 377 °C
650 - 710 °F
RTP Company RTP 1482 Polyethersulfone (PES), Carbon Fiber
Melt Temperature 343 - 377 °C
650 - 710 °F
RTP Company RTP 1499 P X 102560 A Polyphenylenesulfone (PPSU), PTFE Lubricated - Perfluoropolyether Oil
Melt Temperature 343 - 377 °C
650 - 710 °F
RTP Company RTP 1483 HEC Polyethersulfone (PES), Nickel-Coated Carbon Fiber - EMI/RFI/ESD Protection
Melt Temperature 343 - 382 °C
650 - 720 °F
Molding
PolyOne Edgetek® PI-20GM-20CF/000 Polyetherimide (PEI), Carbon/Glass Filled  (discontinued **)
Description/Features:Milled Glass Fiber ReinforcedCarbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 343 - 382 °C
650 - 720 °F
Molding
PolyOne Edgetek® PF-10GF/000 Polysulfone, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 343 - 382 °C
650 - 720 °F
Molding
PolyOne Edgetek® RA-30CF/000 Polyarylsulfone, Carbon Fiber Reinforced  (discontinued **)
Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Melt Temperature 343 - 380 °C
650 - 716 °F
Average value: 364 °C Grade Count:15
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Melt Temperature 343 - 399 °C
649 - 750 °F
Average value: 365 °C Grade Count:12
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Melt Temperature 343 - 385 °C
649 - 725 °F
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensional sta..
Melt Temperature 343 - 399 °C
649 - 750 °F
Solvay Specialty Polymers Veradel® AG-330 Polyethersulfone (PESU)  (Unverified Data**)
Veradel AG-330 is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, dime..
Melt Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 1400 R-5500 Polyphenylsulfone (PPSU), Extrusion Grade
Melt Temperature 343 - 377 °C
650 - 710 °F
RTP Company RTP 1400 TFE 15 Polyethersulfone (PES), PTFE Lubricated
Melt Temperature 343 - 377 °C
650 - 710 °F
RTP Company RTP 1400.5 L MG 15 Polyethersulfone (PES), Glass Fiber - Lubricated - UL94 V-0
Melt Temperature 343 - 377 °C
650 - 710 °F
RTP Company RTP 1401 Polyethersulfone (PES), Glass Fiber
Melt Temperature 343 - 385 °C
650 - 725 °F
RTP Company RTP 3199 X 117877 B Perfluoroalkoxy (PFA), Carbon Nanotube - Electrically Conductive - High Purity
Melt Temperature 343 - 385 °C
650 - 725 °F
RTP Company RTP 3583 Fluorinated Ethylene Propylene (FEP), Carbon Fiber - Preliminary Data