Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
PTS PBT-30GF 30% Glass Fiber Reinforced PBT Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylac® GP74G30 ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
PolyOne Maxxam™ FR QD 818.Y001 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | Conditioned; ASTM D790 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional stabi.. |
|||
Flexural Modulus | 7.60 GPa | 1100 ksi | ISO 178, ASTM D790 |
Nilit Nilamid B G6 FR HF 30% Glass Fiber Reinforced, Flame Retardant PA6 Description: Nilamid B G6 FR HF is a NYLON 6 based flame retardant compound that does not contain any halogen or red phosphorous. It has a good overall mechanical performance, has an excellent price.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D792 |
PTS BLACK PPE/Nylon Alloy 30% Glass Filled Information provided by PTS LLC. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Greene Tweed Arlon® 1160 PEEK, Glass Filled Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Conditioned) Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 420R PBT (Asia Pacific) 30% GR, ex strength/stiffness/dimensional stability; heat resistance. Appliance handles, spotlights, electric motors, etc. Internal mold release.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF35 L UV 35% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 35% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP KF004AL Acetal Homopolymer LNP* THERMOCOMP* KF004AL is a compound based on Acetal Homopolymer resin containing 20% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Techmer ES Electrablend® PA6 04001 BL Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel FiberAdditive: LubricatedFeatures: Electromagnetic Shielding (EMI), Lubricated and Radio Frequency Shielding (RFI.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF33 HS L GY 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Techmer ES HiFill® TPX-HTN-01033 A 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File .. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Techmer ES Plaslube® J-1/CF/10/TF/13/SI/2 NAT PA66 |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Chase Plastics CP Pryme® N330GL (DAM) Nylon 6 (Utility Grade), 30% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 7.60 GPa | 1100 ksi | ASTM-D790 |
Polyram PlusTek RA325G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant 25% glass fiber reinforced, self extinguishing halogen free polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Westlake Plastics Zelux® 30% GF Polycarbonate 30% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Flexural Modulus | 7.60 GPa | 1100 ksi | ASTM D790 |
Adell AL-38 Nylon 66, 40% Glass Reinforced; Mineral Filled Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 7.59 GPa | 1100 ksi | ASTM Test |
BASF Ultramid® 1703-2 BK ND3007 25% Glass Filled PA66 (Dry) Ultramid 1703-2 BK ND3007 is a 25% glass reinforced, heat stabilized injection molding nylon 6/6. |
|||
Flexural Modulus | 7.60 GPa | 1100 ksi | ISO Data |
BASF Ultramid® A27 E 01 PA66 (Conditioned) Ultramid A27 E 01 is a low-viscosity, general-purpose PA66 grade for compounding. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendation ".. |
|||
Flexural Modulus | 7.55 GPa | 1100 ksi | ISO 178 |
BASF Ultramid® B3GM35 BK 60564 40% Glass/Mineral Filled PA6 (Dry) Description: Ultramid B3GM35 BK60564 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade.Applications: industrial articles requiring medium rigidity and.. |
|||
Flexural Modulus | 7.58 GPa | 1100 ksi | ASTM D790 |
Techmer ES Plaslube® J-50/30/TF/15 Polycarbonate, 30% Glass Reinforced, PTFE Lubricated 30% Glass Reinforced, PTFE Lubricated |
|||
Flexural Modulus | 7.58 - 11.3 GPa | 1100 - 1640 ksi | Average value: 8.54 GPa Grade Count:19 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Flexural Modulus | 7.58 - 14.1 GPa | 1100 - 2050 ksi | Average value: 11.0 GPa Grade Count:78 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |