Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.14 - 7.47 J/cm
4.00 - 14.0 ft-lb/in
Average value: 3.36 J/cm Grade Count:17
Overview of materials for Polyphthalamide (PPA), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Unnotched 0.374 - 7.47 J/cm
0.700 - 14.0 ft-lb/in
Average value: 3.28 J/cm Grade Count:13
Overview of materials for Nylon 66, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu..
Izod Impact, Unnotched 4.27 - 7.47 J/cm
8.00 - 14.0 ft-lb/in
Average value: 5.87 J/cm Grade Count:4
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Izod Impact, Unnotched 2.67 - 7.47 J/cm
5.00 - 14.0 ft-lb/in
Average value: 4.98 J/cm Grade Count:34
Overview of materials for Acetal Copolymer + Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Unnotched 1.87 - 7.47 J/cm
3.50 - 14.0 ft-lb/in
Average value: 5.99 J/cm Grade Count:16
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Izod Impact, Unnotched 3.74 - 7.47 J/cm
7.00 - 14.0 ft-lb/in
Average value: 5.91 J/cm Grade Count:13
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Izod Impact, Unnotched 2.80 - 7.45 J/cm

@Temperature -30.0 - -30.0 °C
5.25 - 14.0 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 4.67 J/cm Grade Count:8
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Izod Impact, Unnotched 3.47 - 7.47 J/cm
6.50 - 14.0 ft-lb/in
Average value: 5.62 J/cm Grade Count:6
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..
Izod Impact, Unnotched 1.60 - 7.47 J/cm
3.00 - 14.0 ft-lb/in
Average value: 3.76 J/cm Grade Count:34
Overview of materials for Polypropylene, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum ..