Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 8.00 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 5.00 - 8.00 kJ/m²
2.38 - 3.81 ft-lb/in²
Average value: 5.83 kJ/m² Grade Count:6
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched (ISO) 1.50 - 8.00 kJ/m²

@Temperature -30.0 - -30.0 °C
0.714 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 2.58 kJ/m² Grade Count:6
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Izod Impact, Notched (ISO) 1.50 - 8.00 kJ/m²

@Thickness 4.00 - 4.00 mm
0.714 - 3.81 ft-lb/in²

@Thickness 0.157 - 0.157 in
Average value: 2.58 kJ/m² Grade Count:6
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Izod Impact, Notched (ISO) 5.00 - 8.00 kJ/m²
2.38 - 3.81 ft-lb/in²
Average value: 7.00 kJ/m² Grade Count:4
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched (ISO) 8.00 - 8.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 8.00 kJ/m² Grade Count:1
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Izod Impact, Notched (ISO) 8.00 - 8.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 8.00 kJ/m² Grade Count:1
Overview of materials for Polycarbonate, Foam Grade, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum ..
Izod Impact, Notched (ISO) 1.10 - 8.00 kJ/m²

@Temperature -40.0 - 2.00 °C
0.523 - 3.81 ft-lb/in²

@Temperature -40.0 - 35.6 °F
Average value: 4.02 kJ/m² Grade Count:26
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Izod Impact, Notched (ISO) 5.70 - 8.00 kJ/m²
2.71 - 3.81 ft-lb/in²
Average value: 6.67 kJ/m² Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is ..
Izod Impact, Notched (ISO) 4.00 - 8.00 kJ/m²

@Temperature -30.0 - -30.0 °C
1.90 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.67 kJ/m² Grade Count:3
Overview of materials for Nylon 6, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ..
Izod Impact, Notched (ISO) 1.50 - 8.00 kJ/m²
0.714 - 3.81 ft-lb/in²
Average value: 4.30 kJ/m² Grade Count:30
Overview of materials for Nylon 66, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Izod Impact, Notched (ISO) 5.00 - 8.00 kJ/m²
2.38 - 3.81 ft-lb/in²
Average value: 7.00 kJ/m² Grade Count:3
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Izod Impact, Notched (ISO) 8.00 - 8.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 8.00 kJ/m² Grade Count:1
Overview of materials for Nylon 66, Mineral Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v..
Izod Impact, Notched (ISO) 7.00 - 8.00 kJ/m²
3.33 - 3.81 ft-lb/in²
Type 1, Notch A; ISO 180
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th..
Izod Impact, Notched (ISO) 8.00 - 8.00 kJ/m²

@Temperature -40.0 - -40.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 8.00 kJ/m² Grade Count:2
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma..
Izod Impact, Notched (ISO) 8.00 - 8.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 8.00 kJ/m² Grade Count:1
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
Izod Impact, Notched (ISO) 8.00 - 8.00 kJ/m²

@Temperature -30.0 - -30.0 °C
3.81 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 8.00 kJ/m² Grade Count:1
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Izod Impact, Notched (ISO) 2.10 - 8.00 kJ/m²
0.999 - 3.81 ft-lb/in²
Average value: 4.43 kJ/m² Grade Count:19
Overview of materials for Acrylic, Impact Modified, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values ..
Izod Impact, Notched (ISO) 4.00 - 8.00 kJ/m²

@Temperature -30.0 - 30.0 °C
1.90 - 3.81 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 5.63 kJ/m² Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Izod Impact, Notched (ISO) 5.00 - 8.00 kJ/m²

@Temperature -40.0 - -30.0 °C
2.38 - 3.81 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 6.09 kJ/m² Grade Count:8
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
Izod Impact, Notched (ISO) 5.00 - 8.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.38 - 3.81 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.50 kJ/m² Grade Count:2
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Izod Impact, Notched (ISO) 7.00 - 8.00 kJ/m²
3.33 - 3.81 ft-lb/in²
Higher values are for NT and BK324.; ISO 180/1A
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA)  (Unverified Data**)
Amodel HFFR-4133 is a 33% glass-reinforced, halogen- free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. This ..