Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00350 - 0.00800 cm/cm | 0.00350 - 0.00800 in/in | Average value: 0.00535 cm/cm Grade Count:5 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Linear Mold Shrinkage, Transverse | 0.00150 - 0.00800 cm/cm | 0.00150 - 0.00800 in/in | Average value: 0.00441 cm/cm Grade Count:23 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Linear Mold Shrinkage, Transverse | 0.00700 - 0.00800 cm/cm | 0.00700 - 0.00800 in/in | Average value: 0.00780 cm/cm Grade Count:15 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.00800 cm/cm | 0.00500 - 0.00800 in/in | Average value: 0.00641 cm/cm Grade Count:22 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage, Transverse | 0.000800 - 0.00800 cm/cm | 0.000800 - 0.00800 in/in | Average value: 0.00415 cm/cm Grade Count:30 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00800 cm/cm | 0.00400 - 0.00800 in/in | Average value: 0.00695 cm/cm Grade Count:5 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.00800 cm/cm @Temperature 80.0 - 80.0 °C |
0.00600 - 0.00800 in/in @Temperature 176 - 176 °F |
Average value: 0.00695 cm/cm Grade Count:20 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00800 cm/cm | 0.00400 - 0.00800 in/in | Average value: 0.00677 cm/cm Grade Count:95 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage, Transverse | 0.00580 - 0.00800 cm/cm | 0.00580 - 0.00800 in/in | Average value: 0.00660 cm/cm Grade Count:3 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00800 cm/cm | 0.00400 - 0.00800 in/in | Average value: 0.00580 cm/cm Grade Count:5 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00800 cm/cm | 0.00400 - 0.00800 in/in | Average value: 0.00550 cm/cm Grade Count:4 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00800 cm/cm | 0.00400 - 0.00800 in/in | Average value: 0.00583 cm/cm Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |