Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.00 - 4.50 J/cm² | 14.3 - 21.4 ft-lb/in² | Average value: 3.90 J/cm² Grade Count:10 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Charpy Impact Unnotched | 3.00 - 4.50 J/cm² | 14.3 - 21.4 ft-lb/in² | Average value: 3.50 J/cm² Grade Count:3 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact Unnotched | 1.40 - 4.50 J/cm² | 6.66 - 21.4 ft-lb/in² | Average value: 3.24 J/cm² Grade Count:7 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact Unnotched | 2.50 - 4.50 J/cm² | 11.9 - 21.4 ft-lb/in² | Average value: 3.50 J/cm² Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Charpy Impact Unnotched | 1.00 - 4.50 J/cm² @Temperature -40.0 - -20.0 °C |
4.76 - 21.4 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 2.58 J/cm² Grade Count:12 |
Overview of materials for Nylon 66, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Charpy Impact Unnotched | 2.00 - 4.50 J/cm² | 9.52 - 21.4 ft-lb/in² | ISO 179 |
Bulk Molding Compounds tetra-DUR F 4308 Bulk Molding Compound UL-licensedTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion protection), thermal stabilit.. |
|||
Charpy Impact Unnotched | 2.50 - 4.50 J/cm² @Temperature -30.0 - -30.0 °C |
11.9 - 21.4 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.75 J/cm² Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Charpy Impact Unnotched | 2.00 - 4.50 J/cm² | 9.52 - 21.4 ft-lb/in² | Average value: 3.50 J/cm² Grade Count:5 |
Overview of materials for Acetal Copolymer, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact Unnotched | 4.50 - 4.50 J/cm² @Temperature -30.0 - -30.0 °C |
21.4 - 21.4 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.50 J/cm² Grade Count:1 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Charpy Impact Unnotched | 4.50 - 4.50 J/cm² @Temperature -30.0 - -30.0 °C |
21.4 - 21.4 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.50 J/cm² Grade Count:1 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Charpy Impact Unnotched | 1.50 - 4.50 J/cm² | 7.14 - 21.4 ft-lb/in² | Average value: 3.37 J/cm² Grade Count:7 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Charpy Impact Unnotched | 3.00 - 4.50 J/cm² | 14.3 - 21.4 ft-lb/in² | Average value: 3.50 J/cm² Grade Count:3 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Charpy Impact Unnotched | 4.00 - 4.50 J/cm² @Temperature -30.0 - -20.0 °C |
19.0 - 21.4 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 4.25 J/cm² Grade Count:2 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Charpy Impact Unnotched | 2.00 - 4.50 J/cm² | 9.52 - 21.4 ft-lb/in² | Average value: 3.26 J/cm² Grade Count:15 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |
|||
Charpy Impact Unnotched | 3.00 - 4.50 J/cm² @Temperature -30.0 - -30.0 °C |
14.3 - 21.4 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 3.75 J/cm² Grade Count:4 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |