Processing Properties Metric English Comments
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2200 AR 10  Polyetheretherketone (PEEK) Aramid Fiber 10%  (discontinued **)&
Aramid Fiber 10%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2200 AR 20  Polyetheretherketone (PEEK) Aramid Fiber 20%  (discontinued **)&
Aramid Fiber 20%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2200 AR 35  Polyetheretherketone (PEEK) Aramid Fiber 35%  (discontinued **)&
Aramid Fiber 35%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2201 HF TFE 15  Polyetheretherketone (PEEK) Glass Fiber 10% - PTFE 15% - High Flow &a
Glass Fiber 10% - PTFE 15% - High FlowComments:Glass FiberHigh FlowPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect propertie..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2203 HF Z  Polyetheretherketone (PEEK) Glass Fiber 20% - High Flow - FDA Type &nb
Glass Fiber 20% - High Flow - FDA TypeComments:Glass FiberHigh FlowFDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties...
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2200 LF AR 15 TFE 10  Polyetheretherketone (PEEK) Aramid Fiber 15% - PTFE 10% - Low Flow
Aramid Fiber 15% - PTFE 10% - Low FlowComments:Aramid FiberPTFE LubricatedLow FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect propertie..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2200 LF TFE 20  Polyetheretherketone (PEEK) Low Flow - PTFE 20%  (discontinu
Low Flow - PTFE 20%Comments:Low FlowPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP C..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2203 LF TFE 20  Polyetheretherketone (PEEK) Glass Fiber 20% - PTFE 20% - Low Flow &am
Glass Fiber 20% - PTFE 20% - Low FlowComments:Glass FiberPTFE LubricatedLow FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties...
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2200 LF Z  Polyetheretherketone (PEEK) Low Flow - FDA Type  (discontinued **
Low Flow - FDA TypeComments:Low FlowFDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Com..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2205 TFE 10  Polyetheretherketone (PEEK) Glass Fiber 30% - PTFE 10%  (discon
Glass Fiber 30% - PTFE 10%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provide..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2207 TFE 10  Polyetheretherketone (PEEK) Glass Fiber 40% - PTFE 10%  (discon
Glass Fiber 40% - PTFE 10%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provide..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2289 HF  Polyetheretherketone (PEEK) Carbon Fiber 50% - High Flow  (disconti
Carbon Fiber 50% - High FlowComments:Carbon FiberHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided b..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2289 HM  Polyetheretherketone (PEEK) Carbon Fiber 50% - High Modulus  (disco
Carbon Fiber 50% - High ModulusComments:Carbon FiberHigh ModulusUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information prov..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2285 HEC  Polyetheretherketone (PEEK) Nickel-Coated Carbon Fiber 30% - EMI/ESD &n
Nickel-Coated Carbon Fiber 30% - EMI/ESDComments:EMI/RFI/ESD ProtectionNickel-Coated Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can a..
Processing Temperature 343 - 416 °C
650 - 780 °F
RTP Company RTP 2299 X 68910 A  Polyetheretherketone (PEEK) Long Glass Fiber 40%  (discontin
Long Glass Fiber 40%Comments:Long Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company..
Processing Temperature 343 - 366 °C
650 - 690 °F
RTP Company RTP 1482 HEC  Polyethersulfone (PES) Nickel-Coated Carbon Fiber 15% - EMI/ESD  (
Nickel-Coated Carbon Fiber 15% - EMI/ESDComments:EMI/RFI/ESD ProtectionNickel-Coated Carbon FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can a..
Processing Temperature 343 - 366 °C
650 - 690 °F
RTP Company RTP 1400 A-100  Polyethersulfone (PES) Base Resin  (discontinued **)
Base ResinComments:UnfilledUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for this pro..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2200 GB 30  Polyetheretherketone (PEEK) Glass Bead 30%  (discontinued **)<
Glass Bead 30%Comments:Glass BeadUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2201.3 HF  Polyetheretherketone (PEEK) Glass Fiber 13% - High Flow  (discont
Glass Fiber 13% - High FlowComments:Glass FiberHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by ..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2205 LF Z  Polyetheretherketone (PEEK) Glass Fiber 30% - Low Flow - FDA Type &nbs
Glass Fiber 30% - Low Flow - FDA TypeComments:Glass FiberLow FlowFDA CompliantUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.In..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2282 HF  Polyetheretherketone (PEEK) Carbon Fiber 15% - High Flow  (disconti
Carbon Fiber 15% - High FlowComments:Carbon FiberHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided b..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2282 LF  Polyetheretherketone (PEEK) Carbon Fiber 15% - Low Flow  (discontin
Carbon Fiber 15% - Low FlowComments:Carbon FiberLow FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by ..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2288 LF  Polyetheretherketone (PEEK) Carbon Fiber 45% - Low Flow  (discontin
Carbon Fiber 45% - Low FlowComments:Carbon FiberLow FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by ..
Processing Temperature 343 - 366 °C
650 - 690 °F
Average value: 354 °C Grade Count:6
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Processing Temperature 343 - 366 °C
650 - 690 °F
RTP Company RTP 1400 AR 15  Polyethersulfone (PES) Aramid Fiber 15%  (discontinued **)
Aramid Fiber 15%Comments:Aramid FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data fo..
Processing Temperature 343 - 366 °C
650 - 690 °F
RTP Company RTP 1403 B  Polyethersulfone (PES) Glass Fiber 20%  (discontinued **)
Glass Fiber 20%Comments:Glass FiberUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for ..
Processing Temperature 343 - 366 °C
650 - 690 °F
RTP Company RTP 1400 GB 20  Polyethersulfone (PES) Glass Bead 20%  (discontinued **)
Glass Bead 20%Comments:Glass BeadUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RTP Company.Data for th..
Processing Temperature 343 - 366 °C
650 - 690 °F
RTP Company RTP 1400 N L  Polyethersulfone (PES) Lubricated - High Viscosity  (discontinued
Lubricated - High ViscosityComments:LubricatedHigh ViscosityUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided..
Processing Temperature 343 - 366 °C
650 - 690 °F
RTP Company RTP 1402 N L  Polyethersulfone (PES) Glass Fiber 15% - Lubricated - High Viscosity &n
Glass Fiber 15% - Lubricated - High ViscosityComments:Glass FiberHigh ViscosityLubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect pr..
Processing Temperature 343 - 388 °C
650 - 730 °F
RTP Company RTP 2205 TFE 15  Polyetheretherketone (PEEK) Glass Fiber 30% - PTFE 15%  (discon
Glass Fiber 30% - PTFE 15%Comments:Glass FiberPTFE LubricatedUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provide..