Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.05 - 1.46 g/cc
0.0379 - 0.0527 lb/in³
Average value: 1.34 g/cc Grade Count:126
1.10 - 1.14 g/cc

@Temperature 300 - 300 °C
0.0397 - 0.0412 lb/in³

@Temperature 572 - 572 °F
Average value: 1.11 g/cc Grade Count:3
Filler Content 15.0 - 20.0 %
15.0 - 20.0 %
Average value: 18.8 % Grade Count:28
Water Absorption 0.0200 - 0.350 %
0.0200 - 0.350 %
Average value: 0.170 % Grade Count:62
Moisture Absorption at Equilibrium 0.100 - 0.290 %
0.100 - 0.290 %
Average value: 0.155 % Grade Count:11
Water Absorption at Saturation 0.100 - 0.350 %
0.100 - 0.350 %
Average value: 0.254 % Grade Count:9
Viscosity Test 45.0 - 56.0 cm³/g
45.0 - 56.0 cm³/g
Average value: 50.3 cm³/g Grade Count:8
Maximum Moisture Content 0.0200
0.0200
Average value: 0.0200 Grade Count:5
Linear Mold Shrinkage 0.00100 - 0.0300 cm/cm
0.00100 - 0.0300 in/in
Average value: 0.00332 cm/cm Grade Count:111
Linear Mold Shrinkage, Transverse 0.00250 - 0.00600 cm/cm
0.00250 - 0.00600 in/in
Average value: 0.00456 cm/cm Grade Count:21
Melt Flow 3.00 - 26.0 g/10 min
3.00 - 26.0 g/10 min
Average value: 9.60 g/10 min Grade Count:56
Ash 15.0 - 20.0 %
15.0 - 20.0 %
Average value: 18.3 % Grade Count:3
Mechanical Properties Metric English Comments
Hardness, Rockwell M 81.0 - 93.0
81.0 - 93.0
Average value: 89.8 Grade Count:22
Hardness, Rockwell R 110 - 124
110 - 124
Average value: 120 Grade Count:27
Tensile Strength, Ultimate 45.0 - 118 MPa
6530 - 17100 psi
Average value: 93.7 MPa Grade Count:90
38.0 - 85.0 MPa

@Temperature 60.0 - 120 °C
5510 - 12300 psi

@Temperature 140 - 248 °F
Average value: 58.4 MPa Grade Count:3
Tensile Strength, Yield 47.1 - 120 MPa
6830 - 17400 psi
Average value: 94.9 MPa Grade Count:48
Elongation at Break 1.80 - 25.0 %
1.80 - 25.0 %
Average value: 4.55 % Grade Count:105
1.50 - 2.20 %

@Temperature 60.0 - 120 °C
1.50 - 2.20 %

@Temperature 140 - 248 °F
Average value: 1.72 % Grade Count:2
Elongation at Yield 2.00 - 5.00 %
2.00 - 5.00 %
Average value: 4.19 % Grade Count:10
Modulus of Elasticity 2.10 - 8.27 GPa
305 - 1200 ksi
Average value: 5.57 GPa Grade Count:57
3.80 - 6.00 GPa

@Temperature 60.0 - 120 °C
551 - 870 ksi

@Temperature 140 - 248 °F
Average value: 4.83 GPa Grade Count:2
Flexural Yield Strength 36.0 - 200 MPa
5220 - 29000 psi
Average value: 139 MPa Grade Count:102
Flexural Modulus 2.00 - 8.00 GPa
290 - 1160 ksi
Average value: 5.22 GPa Grade Count:112
3.20 - 3.30 GPa

@Temperature 60.0 - 120 °C
464 - 479 ksi

@Temperature 140 - 248 °F
Average value: 3.27 GPa Grade Count:1
Compressive Yield Strength 96.5 - 124 MPa
14000 - 18000 psi
Average value: 114 MPa Grade Count:8
Izod Impact, Notched 0.392 - 2.16 J/cm
0.735 - 4.04 ft-lb/in
Average value: 1.07 J/cm Grade Count:99
0.500 - 0.550 J/cm

@Temperature -40.0 - -20.0 °C
0.937 - 1.03 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.642 J/cm Grade Count:1
0.600 - 0.800 J/cm

@Temperature -40.0 - 0.000 °C
1.12 - 1.50 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 0.642 J/cm Grade Count:1
0.600 - 0.800 J/cm

@Thickness 3.20 - 3.20 mm
1.12 - 1.50 ft-lb/in

@Thickness 0.126 - 0.126 in
Average value: 0.642 J/cm Grade Count:1
Izod Impact, Unnotched 1.57 - 10.1 J/cm
2.94 - 19.0 ft-lb/in
Average value: 7.43 J/cm Grade Count:29
Izod Impact, Notched (ISO) 10.0 - 13.0 kJ/m²
4.76 - 6.19 ft-lb/in²
Average value: 10.6 kJ/m² Grade Count:12
8.00 - 11.0 kJ/m²

@Temperature -30.0 - -30.0 °C
3.81 - 5.23 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 9.67 kJ/m² Grade Count:3
Charpy Impact Unnotched 3.50 J/cm² - NB
16.7 ft-lb/in² - NB
Average value: 4.50 J/cm² Grade Count:8
3.00 - 5.00 J/cm²

@Temperature -40.0 - -20.0 °C
14.3 - 23.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 4.33 J/cm² Grade Count:2
Charpy Impact, Notched 0.700 - 1.20 J/cm²
3.33 - 5.71 ft-lb/in²
Average value: 0.900 J/cm² Grade Count:7
0.550 - 0.600 J/cm²

@Temperature -20.0 - -20.0 °C
2.62 - 2.86 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 0.590 J/cm² Grade Count:5
Puncture Energy 10.0 - 10.0 J

@Temperature -30.0 - -30.0 °C
7.38 - 7.38 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 10.0 J Grade Count:1
Tensile Creep Modulus, 1 hour 2200 - 10100 MPa
319000 - 1.46e+6 psi
Average value: 5970 MPa Grade Count:3
Tensile Creep Modulus, 1000 hours 1900 - 9600 MPa
276000 - 1.39e+6 psi
Average value: 5430 MPa Grade Count:3
Thermal Properties Metric English Comments
CTE, linear 12.0 - 50.0 µm/m-°C
6.67 - 27.8 µin/in-°F
Average value: 28.7 µm/m-°C Grade Count:33
CTE, linear, Transverse to Flow 49.0 - 65.0 µm/m-°C
27.2 - 36.1 µin/in-°F
Average value: 58.0 µm/m-°C Grade Count:4
Specific Heat Capacity 1.13 - 1.55 J/g-°C
0.270 - 0.370 BTU/lb-°F
Average value: 1.43 J/g-°C Grade Count:4
Thermal Conductivity 0.198 - 0.288 W/m-K
1.37 - 2.00 BTU-in/hr-ft²-°F
Average value: 0.230 W/m-K Grade Count:13
Maximum Service Temperature, Air 80.0 - 145 °C
176 - 293 °F
Average value: 127 °C Grade Count:14
Deflection Temperature at 0.46 MPa (66 psi) 131 - 152 °C
268 - 306 °F
Average value: 145 °C Grade Count:74
Deflection Temperature at 1.8 MPa (264 psi) 122 - 254 °C
252 - 490 °F
Average value: 143 °C Grade Count:109
Electrical Properties Metric English Comments
Electrical Resistivity 1e+05 - 1.00e+17 ohm-cm
1e+05 - 1.00e+17 ohm-cm
Average value: 1.68e+16 ohm-cm Grade Count:58
Surface Resistance 1.00e+9 - 1.00e+16 ohm
1.00e+9 - 1.00e+16 ohm
Average value: 8.68e+14 ohm Grade Count:29
Dielectric Constant 3.05 - 3.30
3.05 - 3.30
Average value: 3.20 Grade Count:32
Dielectric Strength 16.9 - 49.0 kV/mm
430 - 1240 kV/in
Average value: 26.3 kV/mm Grade Count:46
Dissipation Factor 0.000800 - 0.00970
0.000800 - 0.00970
Average value: 0.00518 Grade Count:28
Arc Resistance 30.0 - 179 sec
30.0 - 179 sec
Average value: 116 sec Grade Count:18
Comparative Tracking Index 150 - 249 V
150 - 249 V
Average value: 191 V Grade Count:20