Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 84 Phenolic Formaldehyde Resin, Special Preparation Cylindrical Pellets, High Mechanical Strength
& Phenolic molding compound, organically filled, reinforced with cotton fibers, increased notched impact strength, standardized molding compound.Application areas: Contact support power switch, moldin.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1106-8087/BL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | |
LATI Latishield 85-08A G/20 PES, Steel/Glass Fibers EMI shielding product based on Polyether Sulfone (PES). Steel fibers. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | IS0179 |
Zhejiang Juner 302-G10 10% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner JEPPB005 High Glossy PP Applications: Shell of Air ConditionerInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® F136-DH Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Pebax® 7033 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 70 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: Sport (Football shoe sole, ski top lay.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARNOFORM 300 GF4 POM 20% glass fiber reinforced injection molding grade with very high strength.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARNOFORM 500 UV POM High flow injection molding grade based on Tarnoform 500 modified with carbon black giving best weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAFORM C 520.0 POM Copolymer unreinforced POMInformation provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179 |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
BASF Ultrason S 2010 PSU Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | |
Arkema Group Orgalloy® RS 6030 AT Nylon 6 Alloy, 30% Glass Fiber (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties... |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
CENTROPLAST CENTROMID 6 E FG Polyamide 6 extruded, Food Grade This tough and impact resistant material has good chemical resistance and can be bonded and welded. Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Arnite® TZ6 280 PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Sorona® 3015G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 15% Glass Reinforced Polytrimethylene Terephthalate with Resin Made from Bio-PDO Sorona 3015G NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% ba.. |
|||
Charpy Impact, Notched | 0.550 J/cm² | 2.62 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 101F BKB009 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F BKB009 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled BK 15045 PBT Description: Easy flowing injection molding grade with 15 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg timer dials, toggles, knobs, parts for thermostats, oven-door .. |