Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 1900 - 9600 MPa | 276000 - 1.39e+6 psi | Average value: 5430 MPa Grade Count:3 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |