Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 1900 - 9600 MPa
276000 - 1.39e+6 psi
Average value: 5430 MPa Grade Count:3
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..