Mechanical Properties Metric English Comments
Flexural Yield Strength 68.9 - 200 MPa
10000 - 29000 psi
Average value: 120 MPa Grade Count:19
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Flexural Yield Strength 36.0 - 200 MPa
5220 - 29000 psi
Average value: 139 MPa Grade Count:102
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Flexural Yield Strength 55.2 - 200 MPa
8010 - 29000 psi
Average value: 112 MPa Grade Count:68
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
Flexural Yield Strength 113 - 200 MPa
16400 - 29000 psi
Average value: 160 MPa Grade Count:16
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%..
Flexural Yield Strength 155 - 200 MPa
22500 - 29000 psi
Average value: 178 MPa Grade Count:4
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl..
Flexural Yield Strength 75.0 - 200 MPa

@Temperature -40.0 - 90.0 °C
10900 - 29000 psi

@Temperature -40.0 - 194 °F
Average value: 136 MPa Grade Count:3
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Flexural Yield Strength 62.1 - 200 MPa
9000 - 29000 psi
Average value: 79.9 MPa Grade Count:14
Overview of materials for Nylon 612 with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app..
Flexural Yield Strength 180 - 200 MPa
26100 - 29000 psi
ASTM D790
Chang Chun Plastic PBT3030 30% Glass Fiber Enforced PBT
Information provided by Dowell Trading Company Ltd.
Flexural Yield Strength 165 - 200 MPa
23900 - 29000 psi
Average value: 178 MPa Grade Count:7
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is..
Flexural Yield Strength 16.0 - 200 MPa
2320 - 29000 psi
Average value: 82.1 MPa Grade Count:285
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..