Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.70 - 13.0 kJ/m² | 1.76 - 6.19 ft-lb/in² | Average value: 10.1 kJ/m² Grade Count:20 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Izod Impact, Notched (ISO) | 5.00 - 13.0 kJ/m² @Temperature -40.0 - -30.0 °C |
2.38 - 6.19 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 8.42 kJ/m² Grade Count:19 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched (ISO) | 10.0 - 13.0 kJ/m² | 4.76 - 6.19 ft-lb/in² | Average value: 10.6 kJ/m² Grade Count:12 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Izod Impact, Notched (ISO) | 5.00 - 13.0 kJ/m² @Temperature -30.0 - 120 °C |
2.38 - 6.19 ft-lb/in² @Temperature -22.0 - 248 °F |
Average value: 7.44 kJ/m² Grade Count:6 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 13.0 kJ/m² | 0.952 - 6.19 ft-lb/in² | Average value: 6.07 kJ/m² Grade Count:11 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Izod Impact, Notched (ISO) | 13.0 - 13.0 kJ/m² @Temperature -30.0 - -30.0 °C |
6.19 - 6.19 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 13.0 kJ/m² Grade Count:1 |
Overview of materials for Nylon 612, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app.. |
|||
Izod Impact, Notched (ISO) | 2.00 - 13.0 kJ/m² | 0.952 - 6.19 ft-lb/in² | Average value: 4.38 kJ/m² Grade Count:9 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Notched (ISO) | 0.600 - 13.0 kJ/m² | 0.286 - 6.19 ft-lb/in² | Average value: 8.25 kJ/m² Grade Count:21 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Notched (ISO) | 6.00 - 13.0 kJ/m² @Temperature -40.0 - -20.0 °C |
2.86 - 6.19 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 8.77 kJ/m² Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched (ISO) | 6.00 - 13.0 kJ/m² @Thickness 4.00 - 4.00 mm |
2.86 - 6.19 ft-lb/in² @Thickness 0.157 - 0.157 in |
Average value: 8.77 kJ/m² Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Notched (ISO) | 6.00 - 13.0 kJ/m² @Temperature -30.0 - -20.0 °C |
2.86 - 6.19 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 8.67 kJ/m² Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Izod Impact, Notched (ISO) | 4.50 - 13.0 kJ/m² | 2.14 - 6.19 ft-lb/in² | Average value: 7.57 kJ/m² Grade Count:16 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Izod Impact, Notched (ISO) | 9.50 - 13.0 kJ/m² | 4.52 - 6.19 ft-lb/in² | Average value: 10.7 kJ/m² Grade Count:5 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Izod Impact, Notched (ISO) | 3.00 - 13.0 kJ/m² @Temperature -40.0 - -20.0 °C |
1.43 - 6.19 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 7.82 kJ/m² Grade Count:32 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Izod Impact, Notched (ISO) | 2.94 - 13.0 kJ/m² @Temperature -40.0 - -10.0 °C |
1.40 - 6.19 ft-lb/in² @Temperature -40.0 - 14.0 °F |
Average value: 5.20 kJ/m² Grade Count:10 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched (ISO) | 2.00 - 13.0 kJ/m² @Temperature -40.0 - 0.000 °C |
0.952 - 6.19 ft-lb/in² @Temperature -40.0 - 32.0 °F |
Average value: 5.29 kJ/m² Grade Count:19 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |