Electrical Properties Metric English Comments
Arc Resistance 30.0 - 120 sec
30.0 - 120 sec
Average value: 95.0 sec Grade Count:12
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
Arc Resistance 30.0 - 179 sec
30.0 - 179 sec
Average value: 116 sec Grade Count:18
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Arc Resistance 30.0 - 90.0 sec
30.0 - 90.0 sec
Tungsten Electrodes; ASTM D495
Covestro Makrolon® LQ-2847 Polycarbonate, Lens Quality Optical, Mold Release, UV Stabilized  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..