Polymer Property : Density = 0.0397 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
PolyOne OnForce™ LFT PP-30LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
SABIC Innovative Plastics Lexan® 4251R PPC+PC
High heat polycarbonate copolymer blend with an excellent balance of heat resistance, processability, and impact strength. Available in a range of opaque colors.
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Ravago Manufacturing Americas Hylon® N2000THL Nylon 6 (DAM)
Information provided by Ravago.
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
PTS Trimid® N66-T100HL Toughened, Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
SABIC Innovative Plastics GELOY XP7560 ASA (Europe-Africa-Middle East)
GELOY XP7560 is a general purpose ASA/PC injection moulding grade, available in various colours.
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792B
LyondellBasell Astryn BR33GC Polypropylene Copolymer, Mineral Filled
Key Features: conventional melt flow, high modulus, UV-stabilized, mineral-filled polypropylene copolymer, high rigidity, high impact strength, good dimensional stability, low foggingApplications: k..
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Techmer ES Electrablend® ABS 03008 Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD ProtectionInformation provided by TP Composites, Inc.
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Techmer ES Electrablend® ABS SS5 5% Stainless Steel Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Information provided by TP Composites, Inc.
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Techmer ES HiFill® HDPE GF20 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc.
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Techmer ES Plastiblend® Endura Control
Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceInformation provided by TP Composites, Inc.
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PA (Europe-Africa-Middle East)
NORYL GTX918W is an unfilled global grade, which offers an excellent combination of processability and heat resistance.
Density 1.10 g/cc
0.0397 lb/in³
Solvay SOPROPHOR® FL/60 Surfactant
Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOXYLATED POLYARYLPHENOL PHOSPHATE AMINE SALTSolubility: Soluble in water and most polar solvents. Insoluble in aromat..
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Chase Plastics CP Pryme® A110 ABS, 10% Glass Fiber Reinforced
Features: Glass fiber reinforcementInjection moldingForm: PelletsInformation provided by Chase Plastics.
Density 1.10 g/cc
0.0397 lb/in³
Loctite® 609 General Purpose Retaining Compound
Retainers: Loctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies..
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
EMS-Grivory Grivory® CR 9 PA*
Product description: Grilon CR 9 is a copolyamide with low melting temperature. Grilon CR 9 shows the following features: High flexibility and toughnessGood thermoforming and orientation propertiesH..
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Diamond Polymers NPP30-0500 GF20 20% Glass Filled Black Homopolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, DAM
Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
Density 1.10 g/cc
0.0397 lb/in³
BASF Ultramid® 1C PA6/66 (Conditioned)
Description: Ultramid® 1C forms flexible, scratch-resistant coatings or tough, resilient, abrasion-resistant coverings on plastics, films, nonwovens, fabrics, leather, paper, wood, or metal.Informa..
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM
Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4..
Density 1.10 g/cc

@Temperature 25.0 °C
0.0397 lb/in³

@Temperature 77.0 °F
Liquid
3D Systems Accura® SI 40 Plastic for the SLA® 250 System
Accura 40 "Ar" or "Hc" type materials - for the SLA 250 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing ..
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
LATI LASTIROL TR G/10-V1 ES 10% Glass Fiber Polystyrene (PS) Structural Foam Resin (UL94 V-1)  (discontinued *
Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f..
Density 1.10 g/cc
0.0397 lb/in³
ISO 1183
Sax Polymers SAXAMID 236Q33 Nylon 6.6, Impact Modified
SAXAMID 236Q33 is a impact-modified polyamide 6.6 injection-molding-grade with very good flow properties and outstanding toughness. Even at low temperatures this grade offers super-tough properties...