Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00250 - 0.0170 cm/cm | 0.00250 - 0.0170 in/in | Average value: 0.00629 cm/cm Grade Count:25 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Linear Mold Shrinkage, Transverse | 0.00250 - 0.00600 cm/cm | 0.00250 - 0.00600 in/in | Average value: 0.00456 cm/cm Grade Count:21 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Linear Mold Shrinkage, Transverse | 0.00250 - 0.0135 cm/cm | 0.00250 - 0.0135 in/in | Average value: 0.00644 cm/cm Grade Count:37 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Linear Mold Shrinkage, Transverse | 0.00250 - 0.00500 cm/cm | 0.00250 - 0.00500 in/in | Average value: 0.00387 cm/cm Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is .. |
|||
Linear Mold Shrinkage, Transverse | 0.00250 - 0.0160 cm/cm | 0.00250 - 0.0160 in/in | Average value: 0.00810 cm/cm Grade Count:28 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |
|||
Linear Mold Shrinkage, Transverse | 0.00250 - 0.0300 cm/cm | 0.00250 - 0.0300 in/in | Average value: 0.00686 cm/cm Grade Count:60 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage, Transverse | 0.00250 - 0.00900 cm/cm | 0.00250 - 0.00900 in/in | Average value: 0.00599 cm/cm Grade Count:4 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00250 - 0.00900 cm/cm | 0.00250 - 0.00900 in/in | Average value: 0.00541 cm/cm Grade Count:22 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |