Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00250 - 0.0170 cm/cm
0.00250 - 0.0170 in/in
Average value: 0.00629 cm/cm Grade Count:25
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Linear Mold Shrinkage, Transverse 0.00250 - 0.00600 cm/cm
0.00250 - 0.00600 in/in
Average value: 0.00456 cm/cm Grade Count:21
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Linear Mold Shrinkage, Transverse 0.00250 - 0.0135 cm/cm
0.00250 - 0.0135 in/in
Average value: 0.00644 cm/cm Grade Count:37
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Linear Mold Shrinkage, Transverse 0.00250 - 0.00500 cm/cm
0.00250 - 0.00500 in/in
Average value: 0.00387 cm/cm Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is ..
Linear Mold Shrinkage, Transverse 0.00250 - 0.0160 cm/cm
0.00250 - 0.0160 in/in
Average value: 0.00810 cm/cm Grade Count:28
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
Linear Mold Shrinkage, Transverse 0.00250 - 0.0300 cm/cm
0.00250 - 0.0300 in/in
Average value: 0.00686 cm/cm Grade Count:60
Overview of materials for Polyethersulfone (PES)
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M..
Linear Mold Shrinkage, Transverse 0.00250 - 0.00900 cm/cm
0.00250 - 0.00900 in/in
Average value: 0.00599 cm/cm Grade Count:4
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m..
Linear Mold Shrinkage, Transverse 0.00250 - 0.00900 cm/cm
0.00250 - 0.00900 in/in
Average value: 0.00541 cm/cm Grade Count:22
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..