Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 - 145 °C
176 - 293 °F
Average value: 127 °C Grade Count:14
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..