Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9294 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9348 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9450 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | X; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NX9255 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 12.0 - 500 µm/m-°C | 6.67 - 278 µin/in-°F | Average value: 104 µm/m-°C Grade Count:15 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
CTE, linear | 12.0 - 16.0 µm/m-°C @Temperature -40.0 - 125 °C |
6.67 - 8.90 µin/in-°F @Temperature -40.0 - 257 °F |
X/Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® N4000-2 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-2 is the most established material of Nelco’s product line. This multifunctional epoxy laminate and prepreg system has a long history of use and one of the broadest operating and .. |
|||
CTE, linear | 12.0 - 15.0 µm/m-°C @Temperature -40.0 - 125 °C |
6.67 - 8.33 µin/in-°F @Temperature -40.0 - 257 °F |
IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® N7000-1 Polyimide Laminate and Prepreg The Nelco N7000-1 series of polyimide laminate and prepreg has alow Z-axis expansion and high Tg offering PCB manufacturers consistent board performance and reliability. N7000-1 is a good choice for.. |
|||
CTE, linear | 12.0 - 90.0 µm/m-°C | 6.67 - 50.0 µin/in-°F | Average value: 44.3 µm/m-°C Grade Count:14 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
CTE, linear | 12.0 - 38.0 µm/m-°C | 6.67 - 21.1 µin/in-°F | Average value: 21.1 µm/m-°C Grade Count:36 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear | 12.0 - 30.0 µm/m-°C | 6.67 - 16.7 µin/in-°F | Average value: 18.4 µm/m-°C Grade Count:14 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
CTE, linear | 12.0 - 79.2 µm/m-°C | 6.67 - 44.0 µin/in-°F | Average value: 28.1 µm/m-°C Grade Count:23 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | at Set Pt. |
Ferro CF 7567 Low-Temperature Sealing VITREOUS Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific therm.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 260 °C |
6.67 µin/in-°F @Temperature 500 °F |
|
Ferro EG 2783 Thick Film Glass Glass Type: Pb-B Typical Powder Form: MVG Typical Application: Die Attachment Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 37.8 - 538 °C |
6.66 µin/in-°F @Temperature 100 - 1000 °F |
|
Meehanite HE Heat Resisting Cast Iron Type HE is a freely machinable material in the as-cast condition. Withstands rapid heating and cooling without premature failure, offers good dimensional stability and a good range of strength prop.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 0800 Unsaturated Polyester UP SMC 0800 is a special SMC for applications within househould and kitchenware. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The product .. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 1650 Unsaturated Polyester UP SMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 2300 Unsaturated Polyester UP SMC 2300 is an arc resistance SMC for arc quenching cambers. High fire retardancy SMC for electrical applications .Information Provided by Menzolit |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 0300 Unsaturated Polyester UP SMC 0300 is a low shrink standard SMC providing improved surface quality, reduced shrinkage and warpage. Typical fields of applications are mechanical engineering and electrical industry, where impr.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 100 °C |
6.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals NIMONIC® Alloy 115 A precipitation-hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. It is similar to NIMONIC alloy 105 but has higher levels of aluminum and tit.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | |
Master Bond EP30LTE-LO Dimensionally Stable Low Outgassing Two Part Epoxy Master Bond Polymer System EP30LTE-LO is a thermal shock resistant epoxy resin system with low thermal expansion properties and dimensional stability for high performance bonding, sealing and castin.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 °C |
6.67 µin/in-°F @Temperature 68.0 °F |
MD |
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel.. |
|||
CTE, linear | 12.0 - 15.0 µm/m-°C @Temperature 1000 °C |
6.67 - 8.33 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories HAL-SNA Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | x direction |
Arlon AD255 Woven Glass and PTFE Used in the RF and microwave industries, including base station antennas and BSA feed networks.Information provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | x direction |
Arlon AD320 Glass, PTFE and Micro-Dispersed Ceramic Used in the RF and microwave industries, including base station antennas and BSA feed networks.Information provided by Arlon Materials for Electronics (MED). |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | |
Mo-Sci Corporation GA-40-I Green A Filter Glass Applications: Lead-free NVIS Green A filter glass for incandescent light sources.Information provided by Mo-Sci Corporation. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | |
Mo-Sci Corporation GA-80-N Green Filter Glass Applications: Lead-free NVIS green filter glass for Nichia White LED sources.Information provided by Mo-Sci Corporation. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 °C |
6.67 µin/in-°F @Temperature 68.0 °F |
|
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |