Polymer Property : Linear Mold Shrinkage = 0.0300 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00500 - 0.0300 cm/cm
0.00500 - 0.0300 in/in
Average value: 0.0112 cm/cm Grade Count:34
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar..
Linear Mold Shrinkage 0.00300 - 0.0300 cm/cm
0.00300 - 0.0300 in/in
Average value: 0.00981 cm/cm Grade Count:32
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Linear Mold Shrinkage 0.00500 - 0.0300 cm/cm
0.00500 - 0.0300 in/in
Average value: 0.0160 cm/cm Grade Count:29
Overview of materials for Acetal Copolymer, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values ..
Linear Mold Shrinkage 0.00800 - 0.0300 cm/cm
0.00800 - 0.0300 in/in
Average value: 0.0164 cm/cm Grade Count:29
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va..
Linear Mold Shrinkage 0.00100 - 0.0300 cm/cm
0.00100 - 0.0300 in/in
Average value: 0.00641 cm/cm Grade Count:75
Overview of materials for Polycarbonate, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage 0.00100 - 0.0300 cm/cm
0.00100 - 0.0300 in/in
Average value: 0.00332 cm/cm Grade Count:111
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Linear Mold Shrinkage 0.000 - 0.0300 cm/cm
0.000 - 0.0300 in/in
Average value: 0.00259 cm/cm Grade Count:88
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Linear Mold Shrinkage 0.00100 - 0.0300 cm/cm
0.00100 - 0.0300 in/in
Average value: 0.0118 cm/cm Grade Count:49
Overview of materials for Nylon 66, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage 0.000600 - 0.0300 cm/cm
0.000600 - 0.0300 in/in
Average value: 0.00621 cm/cm Grade Count:175
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Linear Mold Shrinkage 0.00100 - 0.0300 cm/cm
0.00100 - 0.0300 in/in
Average value: 0.00469 cm/cm Grade Count:144
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Linear Mold Shrinkage 0.0100 - 0.0300 cm/cm
0.0100 - 0.0300 in/in
Average value: 0.0221 cm/cm Grade Count:20
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
Linear Mold Shrinkage 0.0150 - 0.0300 cm/cm
0.0150 - 0.0300 in/in
Average value: 0.0176 cm/cm Grade Count:6
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..
Linear Mold Shrinkage 0.000700 - 0.0300 cm/cm
0.000700 - 0.0300 in/in
Average value: 0.00908 cm/cm Grade Count:37
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..