Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.300 - 1.20 J/cm²

@Temperature -40.0 - -40.0 °C
1.43 - 5.71 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 0.750 J/cm² Grade Count:2
Overview of materials for Polyphthalamide (PPA), Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of ..
Charpy Impact, Notched 0.400 - 1.20 J/cm²
1.90 - 5.71 ft-lb/in²
Average value: 0.670 J/cm² Grade Count:17
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Charpy Impact, Notched 0.600 - 1.20 J/cm²
2.86 - 5.71 ft-lb/in²
Average value: 0.933 J/cm² Grade Count:3
Overview of materials for ABS/Polyester Alloy + GF
This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy + GF". Each property range of values reported is minimum and maximum values of appro..
Charpy Impact, Notched 0.300 - 1.20 J/cm²

@Temperature -40.0 - 0.000 °C
1.43 - 5.71 ft-lb/in²

@Temperature -40.0 - 32.0 °F
Average value: 0.633 J/cm² Grade Count:10
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi..
Charpy Impact, Notched 0.700 - 1.20 J/cm²
3.33 - 5.71 ft-lb/in²
Average value: 0.850 J/cm² Grade Count:13
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Charpy Impact, Notched 0.700 - 1.20 J/cm²
3.33 - 5.71 ft-lb/in²
Average value: 0.896 J/cm² Grade Count:13
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Charpy Impact, Notched 0.700 - 1.20 J/cm²
3.33 - 5.71 ft-lb/in²
Average value: 0.900 J/cm² Grade Count:7
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Charpy Impact, Notched 0.400 - 1.20 J/cm²
1.90 - 5.71 ft-lb/in²
Average value: 0.842 J/cm² Grade Count:12
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Charpy Impact, Notched 0.360 - 1.20 J/cm²
1.71 - 5.71 ft-lb/in²
Average value: 0.866 J/cm² Grade Count:10
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Charpy Impact, Notched 0.300 - 1.20 J/cm²
1.43 - 5.71 ft-lb/in²
Average value: 0.688 J/cm² Grade Count:8
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..
Charpy Impact, Notched 0.300 - 1.20 J/cm²
1.43 - 5.71 ft-lb/in²
Average value: 0.730 J/cm² Grade Count:22
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact, Notched 0.200 - 1.20 J/cm²

@Temperature -40.0 - -20.0 °C
0.952 - 5.71 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.566 J/cm² Grade Count:34
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Charpy Impact, Notched 0.500 - 1.20 J/cm²
2.38 - 5.71 ft-lb/in²
Average value: 0.889 J/cm² Grade Count:9
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Charpy Impact, Notched 1.00 - 1.20 J/cm²
4.76 - 5.71 ft-lb/in²
Average value: 1.07 J/cm² Grade Count:7
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Charpy Impact, Notched 0.200 - 1.20 J/cm²
0.952 - 5.71 ft-lb/in²
Average value: 0.520 J/cm² Grade Count:16
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
Charpy Impact, Notched 1.20 - 1.20 J/cm²

@Temperature -30.0 - -30.0 °C
5.71 - 5.71 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.20 J/cm² Grade Count:1
Overview of materials for Nylon 11 with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ..
Charpy Impact, Notched 0.700 - 1.20 J/cm²

@Temperature -30.0 - -20.0 °C
3.33 - 5.71 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.950 J/cm² Grade Count:2
Overview of materials for Nylon 66, 40% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Carbon Fiber Filled". Specific grades with carbon fiber content between 35% and 44% are in..
Charpy Impact, Notched 0.100 - 1.20 J/cm²

@Temperature -30.0 - -20.0 °C
0.476 - 5.71 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.500 J/cm² Grade Count:5
Overview of materials for Nylon 66, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu..
Charpy Impact, Notched 0.300 - 1.20 J/cm²
1.43 - 5.71 ft-lb/in²
Average value: 0.609 J/cm² Grade Count:19
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Charpy Impact, Notched 0.600 - 1.20 J/cm²

@Temperature -30.0 - -20.0 °C
2.86 - 5.71 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.875 J/cm² Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
Charpy Impact, Notched 0.400 - 1.20 J/cm²

@Temperature -30.0 - -20.0 °C
1.90 - 5.71 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.897 J/cm² Grade Count:30
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Charpy Impact, Notched 0.800 - 1.20 J/cm²

@Temperature -40.0 - -30.0 °C
3.81 - 5.71 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.945 J/cm² Grade Count:9
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Charpy Impact, Notched 0.340 - 1.20 J/cm²
1.62 - 5.71 ft-lb/in²
Average value: 0.851 J/cm² Grade Count:14
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
Charpy Impact, Notched 0.400 - 1.20 J/cm²

@Temperature -40.0 - -30.0 °C
1.90 - 5.71 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 0.850 J/cm² Grade Count:9
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
Charpy Impact, Notched 0.200 - 1.20 J/cm²
0.952 - 5.71 ft-lb/in²
Average value: 0.689 J/cm² Grade Count:8
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..
Charpy Impact, Notched 0.600 - 1.20 J/cm²

@Temperature -30.0 - 30.0 °C
2.86 - 5.71 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 0.843 J/cm² Grade Count:20
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..
Charpy Impact, Notched 0.700 - 1.20 J/cm²

@Temperature -30.0 - -20.0 °C
3.33 - 5.71 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.985 J/cm² Grade Count:10
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a..
Copyright © lookpolymers.com All Rights Reserved