Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP620M CPP Film Grade Polypropylene Moplen HP620M is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP620M is suitable for rigid core resin of CPP. Moplen HP620M res.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
PolyMirae Moplen HP450J Stretch/Yarn, Monofilament Grade Polypropylene Moplen HP450J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP450J is a homopolymer typically used by customers in Raffia and Y.. |
|||
Izod Impact, Notched | 0.392 - 4.00 J/cm | 0.735 - 7.49 ft-lb/in | Average value: 1.77 J/cm Grade Count:104 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer
(Unverified Data**) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Izod Impact, Notched | 0.392 - 2.94 J/cm | 0.735 - 5.51 ft-lb/in | Average value: 1.15 J/cm Grade Count:117 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
Izod Impact, Notched | 0.392 - 100 J/cm | 0.735 - 187 ft-lb/in | Average value: 7.09 J/cm Grade Count:113 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOLEFIN® KO133MT20 M/F Reinforced Polypropylene KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2101BF PA66+GF10%, Halogen Free Flame Retardant Feature: Injection Molding, PA66+GF10%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP3200B(W) PA66+MF20%, General Purpose Feature: Injection Molding, PA6+MF20%, General PurposeApplication: E&E (Rice Cooker Housing)Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.735 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HG3200SK2 PP+MF20%, High Gloss Description: Injection Molding, PP+MF20%, High GlossApplication: Electrical & Electronic PartsCAS: 9003-07-0 and 7727-43-7Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® TE5000D PBT+PC Description: Injection Molding, PBT+PC, Good SurfaceApplication: E&E, Automotive (Lamp Housing)CAS No. 24968-12-5 and 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.735 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP3402 PP+MF40% Description: Injection Molding, PP+MF40%, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.35 mm |
>= 0.735 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 1200-211L Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | |
Shinil Chemical SHINSTAT PMMA Electrostatic Control Polymer Injection Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 6.35 mm |
0.735 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® XI-4208 PA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm |
0.735 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® XP-2165BM PPS Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm |
0.735 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-5030FX SAN, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
SK Chemicals SKYPEL G182D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm |
0.735 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® XP-2165BM PPS Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm |
0.735 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tramid® 210F Polyamide, High Productivity Strong with excellent thermal resistance. Abrasion resistance, chemical resistance and oil resistance are excellent.210F is a high productivity grade.Applications:ConnectorsCable tiesHarness clipsT.. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
SK Chemicals SKYPEL G175D General Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm |
0.735 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® TN-1100 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® N602 Nylon 66 Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | |
Zylog Hipolyene® 8001 SGM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
E-Polymers TEKAFIN® PH40FR2 Flame Retardant Heat Resistance Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 3010F Polybutylene terephthalate Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.20 mm |
0.735 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Santron IMS 2006 SAN Resin Very High Rigidity Clear SANInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.392 J/cm | 0.735 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV30G25 POM, 25% Glass Fiber |
|||
Izod Impact, Notched | >= 0.392 J/cm @Thickness 6.35 mm |
>= 0.735 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax CCP PBT 1200-211E Product Description: PBT unreinforced middle viscosity injection molding grade.Characteristics:Excellent electrical propertyExcellent temperature resistance, high heat distortion temperature.Excelle.. |
|||
Izod Impact, Notched | 0.392 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.735 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® D201 PBT Information from Shinkong Synthetic Fibers Corp. |