Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 39.0 - 49.0 kV/mm | 991 - 1240 kV/in | Average value: 44.7 kV/mm Grade Count:3 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Dielectric Strength | 31.0 - 49.0 kV/mm | 787 - 1240 kV/in | Average value: 42.7 kV/mm Grade Count:3 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Dielectric Strength | 16.9 - 49.0 kV/mm | 430 - 1240 kV/in | Average value: 26.3 kV/mm Grade Count:46 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Dielectric Strength | 26.0 - 49.0 kV/mm | 660 - 1240 kV/in | Average value: 37.2 kV/mm Grade Count:8 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |