Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 W-GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179 eU |
Radici Raditer® B RV 100 Polybutylene Terephthalate with 10% Glass fiber Raditer® B RV 100 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properti.. |
|||
Charpy Impact Unnotched | 3.00 - 5.00 J/cm² | 14.3 - 23.8 ft-lb/in² | Average value: 3.50 J/cm² Grade Count:6 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -40.0 °C |
14.3 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL B63 W-KV20 Nylon 6 for injection molding, 20% glass ball reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 3.00 - 4.50 J/cm² | 14.3 - 21.4 ft-lb/in² | Average value: 3.50 J/cm² Grade Count:3 |
Overview of materials for Polycarbonate, Carbon + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + PTFE Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact Unnotched | 3.00 - 1000 J/cm² | 14.3 - 4760 ft-lb/in² | Average value: 8.87 J/cm² Grade Count:69 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1t-7503 Polyamide 6/6T, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | |
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 1/CF/15/HS Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1105-0918/EM/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105-7106 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1105-7107 PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific) Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Styrolux 3G33 SBC Styrolux 3G33 is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion and thermoforming. It offers an outstanding combination of crystal clarity and .. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 30.0 °C |
14.3 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4134 black 9225 PA*-GF30 Product description: Grivory XE 4134 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO polymer designation: PA 10T/X.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature 23.0 °C |
14.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GS 30 HWCP 30% Glass Sphere Filled Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® D 1085 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® 301-G10 PBT Resin 10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/1eU |
CENTROPLAST CENTROLEN PP TV Polypropylene + talc This material is a low density, easily machined plastic that has good damping properties and is reinforced with talc for high rigidity. Applications include components for the electrical industry, h.. |
|||
Charpy Impact Unnotched | 3.00 - 4.00 J/cm² | 14.3 - 19.0 ft-lb/in² | Average value: 3.72 J/cm² Grade Count:8 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Charpy Impact Unnotched | 3.00 J/cm² | 14.3 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eU |
SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East) Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi.. |