Polymer Property : Izod Impact, Notched = 0.937 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Nylene® 609 Nylon 6, Film/Extrusion Grade
Dry as molded. Film grade. Nylene 609 is a high viscosity, extrusion resin recommended for practically all types of extrusion including profile, film, and extrusion coating. It is especially recom..
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
NCMT NanoPAC™ S203 High Performance Polypropylene Nanocomposite
Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Electrical Appliances AutomobileInformation provided by Nano Composi..
Izod Impact, Notched 0.500 J/cm

@Temperature -30.0 °C
0.937 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics GELOY FXW751SK ASA+PC (Asia Pacific)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
fiber
Reliance Industries Polypropylene Impact Copolymer
Typical properties of Reliance - Repol Polypropylene grades. Properties depend on rubber content, presence of nucleating agent, MFIInformation provided by Reliance Industries
Izod Impact, Notched 0.500 J/cm

@Thickness 3.17 mm
0.937 ft-lb/in

@Thickness 0.125 in
ASTM D256
Performance Polymers IPS II PPL-A1050 PEKK (Polyetherketoneketone) Branched Standard Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
Izod Impact, Notched 0.500 J/cm

@Temperature -40.0 °C
0.937 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Shell Carilon® DP P1000 Polyketone  (discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP P1000 is the first in a family of developmental engineering polyketone resins fr..
Izod Impact, Notched 0.500 - 0.500 J/cm

@Temperature -29.0 - -29.0 °C
0.937 - 0.937 ft-lb/in

@Temperature -20.2 - -20.2 °F
Average value: 0.500 J/cm Grade Count:1
Overview of materials for Acetal Copolymer, Silicone Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.500 - 9.77 J/cm
0.937 - 18.3 ft-lb/in
Average value: 7.04 J/cm Grade Count:82
Overview of materials for Polycarbonate, UV Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of a..
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Reliance Industries Repol B250EG Polypropylene
REPOL Polypropylene B250EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly..
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LG Chemical LUPOL HG-3250 High Gloss Polypropylene, 25% Mineral Fillers
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LG Chemical Lupox® SG-4405 Surface Gloss PBT, 40% Glass Fiber/Mineral Reinforced, Dimensional Stability
LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho..
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific)
Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics LNP Lubricomp KFL36XXC Acetal Copolymer (Europe-Africa-Middle East)
LNP* Lubricomp* KFL36 is an Acetal containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched 0.500 J/cm

@Temperature 0.000 °C
0.937 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East)
VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
Izod Impact, Notched 0.500 J/cm

@Temperature -30.0 °C
0.937 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East)
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ISO 180
Wellman Wellamid® 42LH-N Unfilled Nylon 6, Lubricated & Heat Stabilized
Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc.
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram RamTal PM7013G2 Acetal, 10% Glass Fiber
10% Glass fiber reinforced and UV stabilized polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram PlusTek PB350M4 Nylon 6, 20% Mineral Filled
20% mineral filled polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 0.500 J/cm

@Thickness 3.20 mm
0.937 ft-lb/in

@Thickness 0.126 in
ASTM D256
Beijing Chemical Industry KAIFA® 551-GT30S PBT Resin
Glass fiber and mineral filled, flame retardant, low warpage, superior electrical performanceInformation provided by Beijing Chemical Industry Research Institute (Group)
Izod Impact, Notched 0.500 J/cm

@Temperature -20.0 °C
0.937 ft-lb/in

@Temperature -4.00 °F
ASTM D256A
Braskem CP 442 XP Injection Molding Polypropylene
Description: CP 442XP is a medium melt flow rate heterophasic copolymer suitable for injection molding applications. The product combines good stiffness with excellent impact resistance even at sub-..
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
50%RH; ASTM D256
Beijing Ranger Chem BLUESTAR® BS350 Acetal Copolymer
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Izod Impact, Notched 0.500 J/cm

@Temperature -40.0 °C
0.937 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade  (discontinued **)
Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it ..
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Gharda Chemicals Gafone S 1500 Polysulfone (PS)  (discontinued **)
Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec..
Izod Impact, Notched 0.500 J/cm

@Temperature -30.0 °C
0.937 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Europe-Africa-Middle East)
NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance.
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Ineos J50-1000-181 HDPE
A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin c..
Izod Impact, Notched 0.500 J/cm
0.937 ft-lb/in
ASTM D256
Ineos J50-1000-187 HDPE
A high density polyethylene copolymer. It has a narrow molecular weight distribution and is intended for the injection molding of screw caps dedicated to the packaging of still water. This resin con..
Izod Impact, Notched 0.500 - 3.00 J/cm

@Thickness 3.20 - 3.20 mm
0.937 - 5.62 ft-lb/in

@Thickness 0.126 - 0.126 in
Average value: 1.14 J/cm Grade Count:4
Overview of materials for Polypropylene, Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum..
Izod Impact, Notched 0.500 - 3.84408 J/cm

@Temperature -40.0 - 93.3 °C
0.937 - 7.20154 ft-lb/in

@Temperature -40.0 - 200 °F
Average value: 1.61 J/cm Grade Count:5
Overview of materials for Polypropylene with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are i..
Izod Impact, Notched 0.500 J/cm

@Diameter 3.17 mm,
Temperature -20.0 °C
0.937 ft-lb/in

@Diameter 0.125 in,
Temperature -4.00 °F
bar; ASTM D256
BP Amoco Acctuf® 3638 Impact Copolymer Polypropylene  (discontinued **)
Suggested fabrication methods: Injection moldingFeatures: Compounding, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples.