Polymer Property : Thermal Conductivity = 2.00 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.198 - 0.288 W/m-K
1.37 - 2.00 BTU-in/hr-ft²-°F
Average value: 0.230 W/m-K Grade Count:13
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Thermal Conductivity 0.231 - 0.288 W/m-K
1.60 - 2.00 BTU-in/hr-ft²-°F
Average value: 0.269 W/m-K Grade Count:3
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Thermal Conductivity 0.120 - 0.289 W/m-K
0.833 - 2.00 BTU-in/hr-ft²-°F
Average value: 0.129 W/m-K Grade Count:36
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..