Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 KV25 Nylon 6 for injection molding, 25% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® SC699 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® SC699 is a low viscosity acetal homopolymer, lubricated, developed for parts requiring high precision molding in the healthcare industry.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1106/XCF/30 Polyether imide, with carbon fiber, easy flowing Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Electrically conductive, suitable for continuous dis.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179 |
Lucite International Perspexâ„¢ XT IM60 Acrylic Impact Modified Extruded Sheet PERSPEX extruded sheet has a lower molecular weight making it easy to vacuum form and the extrusion process gives excellent thickness tolerance and is economical for long production runs.Information.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | |
LATI Latamid 66 H2 K/50 PA 66, 50% Carbon Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | |
LATI Latilub 75/4-15ST G/30 PBT, 30% Glass Fiber Reinforced, Silicone/PTFE Filled Self-lubricating product based on Polybutylene Terephthalate (PBT). Silicone / PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East) Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO Data, Low Temp |
Styron Magnum™ 2642 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature -20.0 °C |
3.33 ft-lb/in² @Temperature -4.00 °F |
ISO 179/2C |
SABIC Innovative Plastics NORYL GTX GTX830 PPE+PA (Europe-Africa-Middle East) NORYL GTX830 a 30% glass reinforced grade which offers an excellent combination of chemical/heat resistance in combination with stiffness. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature -20.0 °C |
3.33 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ KSR4525 Polypropylene Reactor Elastomer Modified Daplen KSR4525 is a reactor elastomer modified polypropylene intended for injection molding. Daplean KSR4525 is a material with excellent impact/stiffness ratio. The grade is available in natural .. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | IS0179 |
Zhejiang Juner 301-G15 15% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis BS4641 High Density Polyethylene BS4641 is a bimodal high-density polyethylene homopolymer. Because of its excellent organoleptic properties, this grade is especially suitable for blow molding of bottles for food applications. App.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | |
Covestro Apec® HT KU 1-9361 High-Heat Polycarbonate Transparent and opaque shades possible.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated .. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GV 15 HWCP 15% Glass Fiber Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 30.0 °C |
3.33 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HTV-3H1 black 9205 PA6T/6I-GF30 Product description: Grivory HTV-3H1 black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I... |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 30.0 °C |
3.33 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® L 16 nat PA12 Low viscosity unmodified polyamide 12Information provided by EMS Grivory |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® L 20 GM PA12 Product Description: Grilamid L 20 GM is a medium viscosity, heat stabilized polyamide 12 non-reinforced injection molding grade. This product has very good flow characteristics. Special features of.. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® LW9030 BK851 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 BK851 is a 30% glass fiber reinforced black polybutylene terephthalate blend for injection mol.. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal (POM)
(Unverified Data**) Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AL NC010 an unreinforced high viscosity lubricated acetal homopolymer resin containing an advanced system of lub.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Sorona® 3030GV BK001 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV BK001 is a 30% glass reinforced black PTT resin containing 25% renewably sourced ingredients by weight (37% based .. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 30.0 °C |
3.33 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® HT XE 4027 nat PA*-GF30 Product description: Grivory XE 4027 natural is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamid.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® TR 55 PA12/MACMI Product description: Grilamid TR 55 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 55 natural offers outstanding properties.. |
|||
Charpy Impact, Notched | 0.700 J/cm² | 3.33 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARNOFORM 300 POM Basic, fast cycling injection molding grade suitable for many applications.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature -30.0 °C |
3.33 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 30.0 °C |
3.33 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® HT1V-3 HY black 9205 PA6T/6I-GF30 Product description: Grivory HT1V-3 HY black 9205 is a 30% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-3 HY bl.. |
|||
Charpy Impact, Notched | 0.700 J/cm² @Temperature 23.0 °C |
3.33 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Delrin® SC652 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® SC652 is a medium viscosity acetal homopolymer, with an advanced system of lubricants. It is developed for parts requiring low wear, low friction and low squeak noise for the healthcare ind.. |