Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.05 g/cc | 0.0379 lb/in³ | STN EN ISO 1183-1 |
Plastcom PLASTALEN® PQ 81 T 20 Polypropylene reinforced with mineral filler, impact modified Modified PP for injection molding with the content of 20% mineral filler. General application in all industry branches. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Polycasa PS QUINN PS sheets have good optical properties and a brilliant surface. The QUINN PS range contains sheets that are easy to fabricate, to vacuum form, and show a high light transmission (min 88% wavel.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
Polymer Resources ABS-GP1-[color]-3 ABS, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | TA4310A |
Permabond TA4310 Toughened Acrylic Adhesive PERMABOND® TA4310 is a 2-part, 1:1 toughened acrylic adhesive. Its toughening makes it ideal for bonding dissimilar materials where differential thermal expansion and contraction could be an issue... |
|||
Density | 1.05 - 1.53 g/cc | 0.0379 - 0.0553 lb/in³ | Average value: 1.14 g/cc Grade Count:156 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
Global CPP-120 20% CaCO3 Filled, Polypropylene Information provided by Global Polymers Corporation. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
Global TPP-120 20% Talc Filled Polypropylene Information provided by Global Polymers Corporation. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
Momentive Performance Materials RTV102 White Adhesive Sealant, High Strength Paste One-part acetoxy cure. Acetoxy cure silicones are the most commonly used type of RTV materials and are considered GE Silicones' general purpose product line. Typical uses: High strength high perfo.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
LG Chemical 25SPE GPPS Heat resistance, Chemical resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Superior extrusion pr.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM-D792 |
Ineos ABS Lustran® 261 ABS, High-Impact Blending Grade Lustran® ABS 261 resin is a natural, stiffer-flow, virgin blending grade of ABS (acrylonitrile butadiene styrene). It is designed for use with other high-impact ABS resins for drain, waste, and v.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
Styrolution NOVODUR® P2H-AT ABS, Injection Grade Standard injection molding grade, easy flow, high gloss, hard, antistatic.Applications: Telephones, household goods, video and audio industry, office equipment. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Styrolution Terluran® HH-112 Q109 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
Solvay ALKAMULS® S 20 Surfactant Identification: SORBITAN MONOLAURATECAS: 1338 – 39 – 2EINECS : 215 – 663 – 3Solubility: Dispersible in water. Soluble in most polar and aromatic solvents.Available in: Asia Pacif.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
Solvay RHODACAL® LSS-40-A18 Surfactant Description: X High-foaming detergent and emulsifier. Alkali stable. Also used as a foam booster, dispersant and wetter in dishwashing, car- wash products and general- purpose cleanersChemical Name:.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL N110HG PPE+HIPS (Europe-Africa-Middle East) NORYL N110HG is an unfilled material, with a Vicat B/120 of 116°C according ISO 306. NORYL N110HG can be used in applications where high gloss is required. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | LE 4432; ASTM D792 |
Borealis Visico™ LE4423/LE4432 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation Visico LE4423/LE4432 is a black, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a Visico base material.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
Tipco Tipcolene® CR 8229 - 20% Talc/Mineral Reinforced Polypropylene Copolymer Compound with Controlled Rheology 20% Mineral Reinforced, High Flow & Controlled Rheology PP CopolymerApplications: Automotive Door TrimsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
I.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Total PSI 3630 Medium Impact Polystyrene 3630 is an easy flowing, medium impact polystyrene for injection molding. This grade offers a good compromise of flow and softening point allowing for the production of large and complex articles a.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
TPI Porene® ABS-GA800 High Impact ABS Resin Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Cossa Polimeri ESTABLEND PA 3000 ABS / Nylon 6 Blend ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.Easy processing, high surface quality, high chemical resistance, good heat resistanceInformation provided by Cossa Polimeri.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTADIENE 2020 MT Acrylonitrile Butadiene Styrene ABSMedium heat resistance, good impact resistance, good melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO R 1183 D |
Arkema Group Rilsan® Clear G170 Polyamide Rilsan® Clear G170 is a high performance transparent polyamide with outstanding thermal resistance. This grade has been designed for extrusion and injection molding applications and for medical use.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | Typical value for ABS |
Ashley Polymers Ashlene® F242 ABS Flame retardant.Data provided by the manufacturer |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
BASF Polystyrol® 158 K Polystyrene (Global) Heat-resistant, rapid freezing general-purpose grade. Suitable for expanded film and for blending with Styrolux and impact-modified Polystyrol in heat contact applications (e.g. coffee cups).Data w.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ISO 1183 |
Total Lacqrene® 6630 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | |
Loctite® 569 Thread Sealant Thread SealersLoctite® Liquid Thread Sealants seal and secure metal pipes and fittings, filling the space between threaded metal parts, and hardening to prevent leakage. Designed for low and high p.. |
|||
Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON MFD02 PP (Asia Pacific) LNP* Stat-kon* MFD02 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |