Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.198 - 0.288 W/m-K | 1.37 - 2.00 BTU-in/hr-ft²-°F | Average value: 0.230 W/m-K Grade Count:13 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Thermal Conductivity | 0.198 W/m-K | 1.37 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® 1095 Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min15 % Glass fiber reinforcedHigh viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CExtrusionAvailable .. |
|||
Thermal Conductivity | 0.198 W/m-K | 1.37 BTU-in/hr-ft²-°F | Melt |
Covestro Makrolon® GF8002* Polycarbonate, 15% Glass Filled ISO 7391-PC,MR,(,,)-09-9,GF15Formerly Makrolon DP1-1882MVR (300 °C/1.2 kg) 9.5 cm3/10 min15 % Glass fiber reinforcedMedium viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CAva.. |