Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.200 - 26.0 g/10 min | 0.200 - 26.0 g/10 min | Average value: 5.91 g/10 min Grade Count:136 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Melt Flow | 3.00 - 26.0 g/10 min | 3.00 - 26.0 g/10 min | Average value: 9.60 g/10 min Grade Count:56 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Melt Flow | 1.10 - 26.0 g/10 min | 1.10 - 26.0 g/10 min | Average value: 4.90 g/10 min Grade Count:13 |
Overview of materials for Acrylic, UV Stabilized, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Melt Flow | 11.0 - 26.0 g/10 min | 11.0 - 26.0 g/10 min | Average value: 17.7 g/10 min Grade Count:3 |
Overview of materials for ABS/Polyurethane Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyurethane Alloy". Each property range of values reported is minimum and maximum values of appropr.. |