Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 16.7 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
ISO 179-1
Polycasa XT 620 PMMA
QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing..
Charpy Impact Unnotched 3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Qualchem Danamid FCP-40 Polyamide 6, 40% Carbon Fiber
Filled with milled carbon fiber, antistatic and conductiveInformation provided by Qualchem Zrt.
Charpy Impact Unnotched 3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
DuPont Performance Polymers Crastin® SK601 BK851 PBT  (Unverified Data**)
Crastin® SK601 BK851 is a 10% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Charpy Impact Unnotched 3.50 J/cm²

@Temperature -40.0 °C
16.7 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 H-GV25 Nylon 6.6 for injection molding, 25% glass fiber reinforced
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1U
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
Charpy Impact Unnotched 3.50 - 42.5 J/cm²

@Temperature -30.0 - -30.0 °C
16.7 - 202 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 23.5 J/cm² Grade Count:36
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
ISO 179/1eA
Victrex® WG101™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai..
Charpy Impact Unnotched 3.50 - 1000 J/cm²
16.7 - 4760 ft-lb/in²
Average value: 4.50 J/cm² Grade Count:7
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
ISO 179/1eU
Celanese ZENITE 6130L LCP, 30% Glass Reinforced  (Unverified Data**)
Zenite® 6130L is a lubricated 30% glass reinforced LCP resin. It is well suited for use in automotive, electrical/electronic, telecommunications, and aerospace industries.40% glass/mineral reinfo..
Charpy Impact Unnotched 3.50 - 8.70 J/cm²

@Temperature -30.0 - -30.0 °C
16.7 - 41.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 5.29 J/cm² Grade Count:9
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1105-7336/GY7016 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 3-7088-2 Polyamide 6, with carbon fiber and glass fiber, low-warpage, heat stabilized
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall..
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 50/CF/20 Polycarbonate, with carbon fiber, low-warpage
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me..
Charpy Impact Unnotched 3.50 J/cm²

@Temperature -30.0 °C
16.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 50-0828 Polycarbonate, with glass fiber, PTFE, lubricant modified
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi..
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 50-7289 Polycarbonate, with carbon fiber and PTFE
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont..
Charpy Impact Unnotched 3.50 J/cm²

@Temperature -30.0 °C
16.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Lehmann & Voss LUVOCOM® 1/CF/30/TF/13/SI/2/BK Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1105-0904/GN PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1105-0948/YL2 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongationAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Amer..
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
LATI Latiohm 87/26-06 PD01-V1 PC, Flame Retardant
Semiconductive/dissipative product based on Polycarbonate (PC). UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia ..
Charpy Impact Unnotched 3.50 J/cm²

@Temperature -30.0 °C
16.7 ft-lb/in²

@Temperature -22.0 °F
ISO 179/2C
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East)
Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin.
Charpy Impact Unnotched 3.50 J/cm²

@Temperature -30.0 °C
16.7 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
Charpy Impact Unnotched 3.50 J/cm²

@Temperature -30.0 °C
16.7 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS
NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color ..
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
Covestro Makrolon® 9425 Polycarbonate
High viscosity, flame retardant extrusion and injection molding grade with 20% standard glass fibers and easy mold release agent.Information provided by Bayer.As of 1 September 2015, Bayer MaterialS..
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
BASF Procom® D 1153 Polypropylene
Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
ISO179
Beijing Chemical Industry KAIFA® 304-GO0 PBT Resin
Flame retardant, low bleeding, UV-resistantInformation provided by Beijing Chemical Industry Research Institute (Group)
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
BASF Procom® D 1026 Polypropylene
Data was collected by ISO methods and provided by BASF.
Charpy Impact Unnotched 3.50 - 4.00 J/cm²
16.7 - 19.0 ft-lb/in²
Average value: 3.90 J/cm² Grade Count:5
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is ..
Charpy Impact Unnotched 3.50 - 7.50 J/cm²

@Temperature -40.0 - -30.0 °C
16.7 - 35.7 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 5.25 J/cm² Grade Count:10
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..
Charpy Impact Unnotched 3.50 J/cm²
16.7 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1105-7107/BK PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio..