Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 14000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 96.5 MPa
14000 psi
TM R050-38
Resinlab® EP1330 Heat Cure Epoxy Polymer System
Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application..
Compressive Yield Strength 96.5 MPa
14000 psi
TM R050-38
Resinlab® EP1330LV Heat Cure Epoxy Polymer System
Resinlab™ EP1330 and EP1330LV are one part heat cure epoxy polymer systems. They can also be used as a small mass potting or staking compounds, or a dam adhesive in and “dam and fill” application..
Compressive Yield Strength 96.5 - 148 MPa
14000 - 21500 psi
Average value: 114 MPa Grade Count:3
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Compressive Yield Strength 96.5 - 124 MPa
14000 - 18000 psi
Average value: 114 MPa Grade Count:8
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Compressive Yield Strength 96.5 MPa
14000 psi
ASTM D695
Techmer ES Plaslube® J-50/20/TF/15 Polycarbonate, 20% Glass Reinforced, PTFE Lubricated
20% Glass Reinforced, PTFE Lubricated
Compressive Yield Strength 96.5 MPa
14000 psi
Perpendicular to Laminate
TriStar Ultracomp UC-300 Composite Bearing
Ultracomp UC-300 - Similar in construction to UC-200. Containing special fillers that reduce its coefficient of friction, UC-300 is designed to handle higher rotational and linear speeds.This family..
Compressive Yield Strength 96.5 MPa
14000 psi
Perpendicular to Laminate
TriStar Ultracomp UC-400 Composite Bearing
Ultracomp UC-400 - Designed for high loads, low speeds, impact and vibration applications. UC-400 has a MOS2 additive for salt water applications where cathodic reactions could occur. Excellent dry ..