Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 3.00 - 5.00 J/cm² | 14.3 - 23.8 ft-lb/in² | Average value: 3.50 J/cm² Grade Count:6 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact Unnotched | 1.00 - 5.00 J/cm² | 4.76 - 23.8 ft-lb/in² | Average value: 2.69 J/cm² Grade Count:7 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Charpy Impact Unnotched | 2.00 - 5.00 J/cm² | 9.52 - 23.8 ft-lb/in² | Average value: 3.67 J/cm² Grade Count:6 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Charpy Impact Unnotched | 4.00 - 5.00 J/cm² @Temperature -30.0 - -30.0 °C |
19.0 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 4.33 J/cm² Grade Count:3 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Charpy Impact Unnotched | 5.00 - 5.00 J/cm² @Temperature -30.0 - -30.0 °C |
23.8 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.00 J/cm² Grade Count:4 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Charpy Impact Unnotched | 0.400 - 5.00 J/cm² @Temperature -40.0 - -20.0 °C |
1.90 - 23.8 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 2.36 J/cm² Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Charpy Impact Unnotched | 3.00 - 5.00 J/cm² @Temperature -40.0 - -20.0 °C |
14.3 - 23.8 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.33 J/cm² Grade Count:2 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Charpy Impact Unnotched | 5.00 - 5.00 J/cm² @Temperature -30.0 - -30.0 °C |
23.8 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.00 J/cm² Grade Count:1 |
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Charpy Impact Unnotched | 2.00 - 5.00 J/cm² @Temperature -30.0 - -20.0 °C |
9.52 - 23.8 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 4.00 J/cm² Grade Count:11 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 5.00 - 5.00 J/cm² @Temperature -30.0 - -30.0 °C |
23.8 - 23.8 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 5.00 J/cm² Grade Count:4 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Charpy Impact Unnotched | 2.50 - 5.00 J/cm² | 11.9 - 23.8 ft-lb/in² | Average value: 3.12 J/cm² Grade Count:5 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Charpy Impact Unnotched | 2.80 - 5.00 J/cm² | 13.3 - 23.8 ft-lb/in² | Average value: 4.14 J/cm² Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Charpy Impact Unnotched | 3.50 - 5.00 J/cm² @Temperature -40.0 - -30.0 °C |
16.7 - 23.8 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 4.05 J/cm² Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
Charpy Impact Unnotched | 2.00 - 5.00 J/cm² | 9.52 - 23.8 ft-lb/in² | Average value: 3.80 J/cm² Grade Count:8 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |
|||
Charpy Impact Unnotched | 2.20 - 5.00 J/cm² | 10.5 - 23.8 ft-lb/in² | Average value: 3.55 J/cm² Grade Count:15 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |
|||
Charpy Impact Unnotched | 1.90 - 5.00 J/cm² @Temperature -30.0 - 30.0 °C |
9.04 - 23.8 ft-lb/in² @Temperature -22.0 - 86.0 °F |
Average value: 3.19 J/cm² Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |
|||
Charpy Impact Unnotched | 2.50 - 5.00 J/cm² | 11.9 - 23.8 ft-lb/in² | Average value: 3.50 J/cm² Grade Count:9 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |