Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Nylon 66, 10% Glass Fiber Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 10% Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 66, 10% Glass Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.09 - 1.70 g/cc
0.0394 - 0.0614 lb/in³
Average value: 1.23 g/cc Grade Count:215
1.03 - 1.03 g/cc

@Temperature 295 - 295 °C
0.0372 - 0.0372 lb/in³

@Temperature 563 - 563 °F
Average value: 1.03 g/cc Grade Count:1
Filler Content 5.00 - 15.0 %
5.00 - 15.0 %
Average value: 11.3 % Grade Count:47
Water Absorption 0.350 - 8.00 %
0.350 - 8.00 %
Average value: 1.78 % Grade Count:110
2.60 - 2.80 %

@Temperature 70.0 - 70.0 °C
2.60 - 2.80 %

@Temperature 158 - 158 °F
Average value: 2.70 % Grade Count:2
Moisture Absorption at Equilibrium 1.80 - 3.00 %
1.80 - 3.00 %
Average value: 2.17 % Grade Count:27
Water Absorption at Saturation 5.50 - 8.00 %
5.50 - 8.00 %
Average value: 6.97 % Grade Count:12
Viscosity Test 140 - 150 cm³/g
140 - 150 cm³/g
Average value: 147 cm³/g Grade Count:4
Linear Mold Shrinkage 0.00100 - 0.0550 cm/cm
0.00100 - 0.0550 in/in
Average value: 0.00760 cm/cm Grade Count:191
Linear Mold Shrinkage, Transverse 0.00500 - 0.0150 cm/cm
0.00500 - 0.0150 in/in
Average value: 0.0102 cm/cm Grade Count:32
Melt Flow 1.00 - 80.0 g/10 min
1.00 - 80.0 g/10 min
Average value: 25.0 g/10 min Grade Count:9
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70.0 - 95.0
70.0 - 95.0
Average value: 86.5 Grade Count:12
Hardness, Rockwell R 95.0 - 122
95.0 - 122
Average value: 116 Grade Count:81
Hardness, Shore D 73.0 - 81.0
73.0 - 81.0
Average value: 76.0 Grade Count:3
Ball Indentation Hardness 102 - 165 MPa
14800 - 23900 psi
Average value: 139 MPa Grade Count:5
Tensile Strength, Ultimate 29.6 - 175 MPa
4300 - 25400 psi
Average value: 96.8 MPa Grade Count:156
35.0 - 70.0 MPa

@Temperature 60.0 - 150 °C
5080 - 10200 psi

@Temperature 140 - 302 °F
Average value: 53.8 MPa Grade Count:1
57.5 - 57.5 MPa

@Temperature 130 - 175 °C
8340 - 8340 psi

@Temperature 266 - 347 °F
Average value: 53.8 MPa Grade Count:1
57.5 - 57.5 MPa

@Time 1.80e+7 - 7.20e+7 sec
8340 - 8340 psi

@Time 5000 - 20000 hour
Average value: 53.8 MPa Grade Count:1
Tensile Strength, Yield 10.3 - 252 MPa
1500 - 36500 psi
Average value: 104 MPa Grade Count:75
Elongation at Break 1.50 - 20.0 %
1.50 - 20.0 %
Average value: 4.91 % Grade Count:190
6.50 - 12.0 %

@Temperature 60.0 - 150 °C
6.50 - 12.0 %

@Temperature 140 - 302 °F
Average value: 10.1 % Grade Count:1
Elongation at Yield 2.75 - 8.00 %
2.75 - 8.00 %
Average value: 4.30 % Grade Count:16
4.00 - 8.00 %

@Temperature 60.0 - 150 °C
4.00 - 8.00 %

@Temperature 140 - 302 °F
Average value: 6.63 % Grade Count:1
Modulus of Elasticity 1.79 - 36.5 GPa
260 - 5290 ksi
Average value: 4.98 GPa Grade Count:78
1.50 - 6.543 GPa

@Temperature -40.0 - 150 °C
218 - 949.0 ksi

@Temperature -40.0 - 302 °F
Average value: 3.47 GPa Grade Count:3
Flexural Yield Strength 43.0 - 407 MPa
6240 - 59000 psi
Average value: 149 MPa Grade Count:173
Flexural Modulus 0.483 - 36.2 GPa
70.0 - 5250 ksi
Average value: 4.87 GPa Grade Count:205
Compressive Yield Strength 89.6 - 172 MPa
13000 - 24900 psi
Average value: 122 MPa Grade Count:3
Shear Modulus >= 0.0971 GPa

@Temperature -50.0 - 250 °C
>= 14.1 ksi

@Temperature -58.0 - 482 °F
Average value: 0.632 GPa Grade Count:2
Shear Strength 42.0 - 76.0 MPa
6090 - 11000 psi
Average value: 58.9 MPa Grade Count:7
Izod Impact, Notched 0.320 - 2.94 J/cm
0.600 - 5.50 ft-lb/in
Average value: 0.876 J/cm Grade Count:151
0.69407 - 0.69407 J/cm

@Temperature -40.0 - -40.0 °C
1.3003 - 1.3003 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.05 J/cm Grade Count:1
1.0678 - 1.0678 J/cm

@Temperature -40.0 - -40.0 °C
2.0004 - 2.0004 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 1.05 J/cm Grade Count:9
1.0678 - 1.0678 J/cm

@Thickness 3.17 - 3.17 mm
2.0004 - 2.0004 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 1.05 J/cm Grade Count:9
Izod Impact, Unnotched 0.481 - 5340 J/cm
0.900 - 10000 ft-lb/in
Average value: 4.50 J/cm Grade Count:45
Izod Impact, Notched (ISO) 3.00 - 18.0 kJ/m²
1.43 - 8.57 ft-lb/in²
Average value: 8.38 kJ/m² Grade Count:42
3.00 - 12.0 kJ/m²

@Temperature -40.0 - -20.0 °C
1.43 - 5.71 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 5.62 kJ/m² Grade Count:17
Izod Impact, Unnotched (ISO) 35.0 - 100 kJ/m²
16.7 - 47.6 ft-lb/in²
Average value: 58.9 kJ/m² Grade Count:12
28.0 - 90.0 kJ/m²

@Temperature -30.0 - -30.0 °C
13.3 - 42.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 52.3 kJ/m² Grade Count:6
Charpy Impact Unnotched 2.00 J/cm² - NB
9.52 ft-lb/in² - NB
Average value: 5.25 J/cm² Grade Count:44
2.40 - 9.00 J/cm²

@Temperature -40.0 - -20.0 °C
11.4 - 42.8 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 4.51 J/cm² Grade Count:28
Charpy Impact, Notched 0.400 - 1.80 J/cm²
1.90 - 8.57 ft-lb/in²
Average value: 0.840 J/cm² Grade Count:51
0.200 - 1.20 J/cm²

@Temperature -40.0 - -20.0 °C
0.952 - 5.71 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.566 J/cm² Grade Count:34
Tensile Creep Modulus, 1 hour 3100 - 4030 MPa
450000 - 585000 psi
Average value: 3430 MPa Grade Count:4
Tensile Creep Modulus, 1000 hours 2200 - 3180 MPa
319000 - 461000 psi
Average value: 2520 MPa Grade Count:4
Electrical Properties Metric English Comments
Electrical Resistivity 10.0 - 1.00e+15 ohm-cm
10.0 - 1.00e+15 ohm-cm
Average value: 4.60e+14 ohm-cm Grade Count:89
Surface Resistance 10.0 - 1.00e+15 ohm
10.0 - 1.00e+15 ohm
Average value: 5.40e+13 ohm Grade Count:31
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.62 sec Grade Count:5
Dielectric Constant 3.10 - 9.80
3.10 - 9.80
Average value: 4.46 Grade Count:16
Dielectric Strength 17.3 - 111 kV/mm
440 - 2820 kV/in
Average value: 26.2 kV/mm Grade Count:59
Dissipation Factor 0.00650 - 0.250
0.00650 - 0.250
Average value: 0.0515 Grade Count:17
Dielectric Loss Index 0.0150 - 0.150
0.0150 - 0.150
Average value: 0.0825 Grade Count:4
Arc Resistance 0.000 - 120 sec
0.000 - 120 sec
Average value: 81.9 sec Grade Count:5