Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 9.52 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
Polycasa Acryl® G 55 Acrylic, Injection Molding Grade
Injection molding grade for very long flow paths, as well as thin-walled parts.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -40.0 °C
9.52 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 HH-KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.00 J/cm² - NB
9.52 ft-lb/in² - NB
Average value: 6.08 J/cm² Grade Count:32
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Charpy Impact Unnotched 2.00 J/cm² - NB
9.52 ft-lb/in² - NB
Average value: 3.95 J/cm² Grade Count:44
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eU
Celanese Impet® 2700 GV1/20 PET, 20% Glass Reinforced  (Unverified Data**)
Polyethylene terephthalate, 20 % glass fibre reinforced, high flowability, excellent gloss, high modulus20% glass fiber reinforcedInformation provided by Celanese
Charpy Impact Unnotched 2.00 - 5.50 J/cm²
9.52 - 26.2 ft-lb/in²
Average value: 3.82 J/cm² Grade Count:14
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -40.0 °C
9.52 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179-1/1eU
Quadrant EPP Semitron® ESd 410C PEI, static dissipative, extruded (ISO Data)
Having an excellent mechanical performance up to 210 °C, Semitron ESd 410C provides ESd-solutions at higher temperatures. Additionally, Semitron ESd 410C exhibits excellent dimensional stability (l..
Charpy Impact Unnotched 2.00 J/cm² - NB

@Temperature -40.0 - -20.0 °C
9.52 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 6.01 J/cm² Grade Count:17
Overview of materials for Nylon 66, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum ..
Charpy Impact Unnotched 2.00 - 9.00 J/cm²
9.52 - 42.8 ft-lb/in²
Average value: 4.88 J/cm² Grade Count:24
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5 BK PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301-7293/GN PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
edgewise; ISO 179 1eU
Lehmann & Voss LUVOCOM® 1301-8077 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricity.S..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
flatwise; ISO 179 1fU
Lehmann & Voss LUVOCOM® 1850/TF/30 PBT, with PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eU
Lucite International Diakon® CMG334V Acrylic Polymer
Information provided by Lucite International
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
LATI Latene® 7H2W TR/40 PP Homopolymer, Mineral Reinforced, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Metal stabilized. Mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pr..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
LATI Latene® 11 MDT05-01 PP Homopolymer
Polypropylene homopolymer (PPh) based compound. Magnetic detectable filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
LATI Latilub 73/13-15T G/15 POM, 15% Glass Fiber Reinforced, PTFE Filled
Self-lubricating product based on Polyoxymethylene (POM). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
LATI Latiohm 73-09 PD01 G/20 POM, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyoxymethylene (POM). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati ..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
SABIC Innovative Plastics LNP THERMOCOMP Noryl_PCN2910 PPE+PS (Asia Pacific)
35% Glass/Mica filled. High modulus and tight tolerance molding for the chassis market.
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC)
TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Evonik Corporation Plexiglas® 6N PMMA Molding Compound
Description: PLEXIGLAS® 6N is a molding compound based on polymethyl methacrylate (PMMA). The special properties of PLEXIGLAS® 6N are:good flowhigh mechanical strength, surface hardness and abrasi..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179
CP-Polymer-Technik Wellamid® 6600 GS 20 HWCP 20% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry
Information provided by CP-Polymer-Technik GmbH & Co. KG
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese CELANEX 3200-2 PBT, 15% Glass Reinforced
Celanex 3200-2 is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability. Celanex 3200-2 contains an internal lubricant.In..
Charpy Impact Unnotched 2.00 J/cm²

@Temperature -30.0 °C
9.52 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Celanese CELANEX 3200-2FC PBT, 15% Glass Reinforced
Celanex 3200-2FC is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability for use in food contact applications. Celanex 3..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179/1eU
Celanese Celanex® 3200 PBT, 15% Glass Reinforced
Celanex 3200 is a general purpose, 15% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.To avoid hydrolytic degradation during processing, ..
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
Conditioned; ISO 179/IeU
Addiplast Addilene J 490 M40S Flame Retardant Polypropylene, 40% Mineral Filled
Flame retardant, mineral filled, with halogensInformation provided by Addiplast.
Charpy Impact Unnotched 2.00 J/cm²
9.52 ft-lb/in²
ISO 179-1
Celanese Coolpoly® D3606 Thermally Conductive Polyamide 4,6  (discontinued **)
CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows ..
Charpy Impact Unnotched 2.00 - 3.00 J/cm²
9.52 - 14.3 ft-lb/in²
Average value: 2.50 J/cm² Grade Count:3
Overview of materials for Acetal Copolymer + Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of ..
Charpy Impact Unnotched 2.00 - 4.00 J/cm²

@Temperature -40.0 - -30.0 °C
9.52 - 19.0 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 3.07 J/cm² Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
Copyright © lookpolymers.com All Rights Reserved