Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.60 - 5340 J/cm | 3.00 - 10000 ft-lb/in | Average value: 2.14 J/cm Grade Count:10 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Izod Impact, Unnotched | 6.41 - 5340 J/cm | 12.0 - 10000 ft-lb/in | Average value: 12.8 J/cm Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Izod Impact, Unnotched | 4.80 - 5340 J/cm | 8.99 - 10000 ft-lb/in | Average value: 4.80 J/cm Grade Count:3 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched | 6.94 - 5340 J/cm | 13.0 - 10000 ft-lb/in | Average value: 6.94 J/cm Grade Count:14 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Unnotched | 10.7 - 5340 J/cm | 20.0 - 10000 ft-lb/in | Average value: 16.4 J/cm Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Izod Impact, Unnotched | 3.20 - 5340 J/cm | 6.00 - 10000 ft-lb/in | Average value: 10.5 J/cm Grade Count:13 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched | 11.7 - 5340 J/cm | 22.0 - 10000 ft-lb/in | Average value: 13.4 J/cm Grade Count:7 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched | 7.85 - 5340 J/cm | 14.7 - 10000 ft-lb/in | Average value: 8.50 J/cm Grade Count:5 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Izod Impact, Unnotched | 2.40 - 5340 J/cm | 4.50 - 10000 ft-lb/in | Average value: 6.94 J/cm Grade Count:13 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Unnotched | 3.20 - 5340 J/cm | 5.99 - 10000 ft-lb/in | Average value: 8.36 J/cm Grade Count:10 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Unnotched | 0.200 - 5340 J/cm | 0.375 - 10000 ft-lb/in | Average value: 5.80 J/cm Grade Count:44 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Izod Impact, Unnotched | 0.534 - 5340 J/cm | 1.00 - 10000 ft-lb/in | Average value: 9.81 J/cm Grade Count:19 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Izod Impact, Unnotched | 3.20 - 5340 J/cm | 6.00 - 10000 ft-lb/in | Average value: 8.92 J/cm Grade Count:19 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Izod Impact, Unnotched | 2.14 - 5340 J/cm | 4.00 - 10000 ft-lb/in | Average value: 7.68 J/cm Grade Count:18 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Izod Impact, Unnotched | 4.27 - 5340 J/cm | 8.00 - 10000 ft-lb/in | Average value: 8.81 J/cm Grade Count:4 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Izod Impact, Unnotched | 1.39 - 5340 J/cm | 2.60 - 10000 ft-lb/in | Average value: 11.7 J/cm Grade Count:35 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Izod Impact, Unnotched | 0.481 - 5340 J/cm | 0.900 - 10000 ft-lb/in | Average value: 4.50 J/cm Grade Count:45 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Izod Impact, Unnotched | 4.64 - 5340 J/cm | 8.69 - 10000 ft-lb/in | Average value: 8.60 J/cm Grade Count:47 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Izod Impact, Unnotched | 2.14 - 5340 J/cm | 4.00 - 10000 ft-lb/in | Average value: 3.99 J/cm Grade Count:6 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Izod Impact, Unnotched | 5.34 - 5340 J/cm | 10.0 - 10000 ft-lb/in | Average value: 7.32 J/cm Grade Count:9 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Izod Impact, Unnotched | 0.300 - 5340 J/cm | 0.562 - 10000 ft-lb/in | Average value: 0.300 J/cm Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |
|||
Izod Impact, Unnotched | 9.08 - 5340 J/cm | 17.0 - 10000 ft-lb/in | Average value: 9.08 J/cm Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Izod Impact, Unnotched | 3.47 - 5340 J/cm | 6.50 - 10000 ft-lb/in | Average value: 6.69 J/cm Grade Count:47 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Unnotched | 7.35 - 5340 J/cm | 13.8 - 10000 ft-lb/in | Average value: 12.2 J/cm Grade Count:46 |
Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Izod Impact, Unnotched | 2.14 - 5340 J/cm | 4.00 - 10000 ft-lb/in | Average value: 12.1 J/cm Grade Count:59 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Izod Impact, Unnotched | 2.67 - 5340 J/cm | 5.00 - 10000 ft-lb/in | Average value: 5.94 J/cm Grade Count:24 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Unnotched | 0.801 - 5340 J/cm | 1.50 - 10000 ft-lb/in | Average value: 8.47 J/cm Grade Count:46 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Unnotched | 6.67 - 5340 J/cm | 12.5 - 10000 ft-lb/in | Average value: 9.98 J/cm Grade Count:6 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Izod Impact, Unnotched | 1.33 - 5340 J/cm | 2.50 - 10000 ft-lb/in | Average value: 4.39 J/cm Grade Count:41 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |
|||
Izod Impact, Unnotched | 1.60 - 5340 J/cm | 3.00 - 10000 ft-lb/in | Average value: 4.74 J/cm Grade Count:42 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |