Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 2.40 J/cm² @Temperature -40.0 °C |
11.4 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 FK 2010 Nylon 6.6 for injection molding, 20% glass fiber and 10% glass ball reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.40 J/cm² @Temperature -40.0 °C |
11.4 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 HH-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.40 J/cm² | 11.4 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 HH-KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.40 J/cm² | 11.4 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 HH-KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.40 J/cm² @Temperature -40.0 °C |
11.4 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL A63 SG30 Nylon 6.6 for injection molding, 30% mineral filled Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.40 J/cm² @Temperature -40.0 °C |
11.4 ft-lb/in² @Temperature -40.0 °F |
DIN 53453 |
Nilit FRIANYL C73 H-GV30 Nylon 6.6/6 for injection molding, 30% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO 179/1eU |
Nilit FRIANYL A63 BR80 Nylon 6.6 for injection molding, 80% bronze filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.40 J/cm² | 11.4 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.40 J/cm² | 11.4 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 KV20 Nylon 6.6 for injection molding, 20% glass ball reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Nilit FRIANYL A63 V0 G5 Nylon 6.6 for injection molding, 25% glass fiber reinforced Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact Unnotched | 2.40 J/cm² - NB | 11.4 ft-lb/in² - NB | Average value: 16.1 J/cm² Grade Count:94 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 2.40 J/cm² - NB @Temperature -40.0 - 30.0 °C |
11.4 ft-lb/in² - NB @Temperature -40.0 - 86.0 °F |
Average value: 5.44 J/cm² Grade Count:35 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Charpy Impact Unnotched | 2.40 - 9.00 J/cm² @Temperature -40.0 - -20.0 °C |
11.4 - 42.8 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.51 J/cm² Grade Count:28 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Charpy Impact Unnotched | 2.40 J/cm² | 11.4 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1301-8457 PPS, linear, with carbon fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo.. |
|||
Charpy Impact Unnotched | 2.40 J/cm² | 11.4 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-8491 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab.. |
|||
Charpy Impact Unnotched | 2.40 J/cm² | 11.4 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1850-7557 PBT, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour, self-lubricating, for highest tribologic needs.Low warpag.. |
|||
Charpy Impact Unnotched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East) VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto.. |
|||
Charpy Impact Unnotched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East) VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto.. |
|||
Charpy Impact Unnotched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DSM Arnite® B600SE PBT FR Flame Retardant |
|||
Charpy Impact Unnotched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO 179 |
Chi Mei Kibisan® PN-127H SAN Chemical Resistant |
|||
Charpy Impact Unnotched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 70GB30HSL NC010 Nylon 66 Zytel® 70GB30HSL NC010 is a 30% glass bead reinforced heat stabilized polyamide 66 resin.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 2.40 J/cm² @Temperature -30.0 °C |
11.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultradur B 4040 G4 LS High Speed BK15029 20% Glass Filled PBT/PET |