Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.0 - 70.0 MPa
5950 - 10200 psi
Average value: 55.1 MPa Grade Count:10
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report..
Tensile Strength, Ultimate 15.0 - 70.0 MPa
2180 - 10200 psi
Average value: 33.4 MPa Grade Count:13
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
Tensile Strength, Ultimate 35.0 - 70.0 MPa

@Temperature 60.0 - 150 °C
5080 - 10200 psi

@Temperature 140 - 302 °F
Average value: 53.8 MPa Grade Count:1
Overview of materials for Nylon 66, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Tensile Strength, Ultimate 25.0 - 70.0 MPa

@Temperature 60.0 - 150 °C
3630 - 10200 psi

@Temperature 140 - 302 °F
Average value: 50.9 MPa Grade Count:2
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Tensile Strength, Ultimate 51.7 - 70.0 MPa
7500 - 10200 psi
Average value: 61.7 MPa Grade Count:6
Overview of materials for PC/ABS + Stainless Steel
This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro..
Tensile Strength, Ultimate 20.0 - 70.0 MPa

@Temperature 60.0 - 120 °C
2900 - 10200 psi

@Temperature 140 - 248 °F
Average value: 44.2 MPa Grade Count:2
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Tensile Strength, Ultimate 50.0 - 70.0 MPa
7250 - 10200 psi
ASTM D638
Chang Chun Plastic PBT2000 Fire Retardant PBT
Information provided by Dowell Trading Company Ltd.
Tensile Strength, Ultimate 50.0 - 70.0 MPa
7250 - 10200 psi
ASTM D638
Chang Chun Plastic PBT2100 Fire Retardant PBT
Information provided by Dowell Trading Company Ltd.