Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 41.0 - 70.0 MPa | 5950 - 10200 psi | Average value: 55.1 MPa Grade Count:10 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report.. |
|||
Tensile Strength, Ultimate | 15.0 - 70.0 MPa | 2180 - 10200 psi | Average value: 33.4 MPa Grade Count:13 |
Overview of materials for Polypropylene, Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu.. |
|||
Tensile Strength, Ultimate | 35.0 - 70.0 MPa @Temperature 60.0 - 150 °C |
5080 - 10200 psi @Temperature 140 - 302 °F |
Average value: 53.8 MPa Grade Count:1 |
Overview of materials for Nylon 66, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Tensile Strength, Ultimate | 25.0 - 70.0 MPa @Temperature 60.0 - 150 °C |
3630 - 10200 psi @Temperature 140 - 302 °F |
Average value: 50.9 MPa Grade Count:2 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Ultimate | 51.7 - 70.0 MPa | 7500 - 10200 psi | Average value: 61.7 MPa Grade Count:6 |
Overview of materials for PC/ABS + Stainless Steel This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro.. |
|||
Tensile Strength, Ultimate | 20.0 - 70.0 MPa @Temperature 60.0 - 120 °C |
2900 - 10200 psi @Temperature 140 - 248 °F |
Average value: 44.2 MPa Grade Count:2 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Tensile Strength, Ultimate | 32.4 - 70.3 MPa | 4700 - 10200 psi | Average value: 59.1 MPa Grade Count:13 |
Overview of materials for Acrylic, UV Stabilized, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Tensile Strength, Ultimate | 50.0 - 70.0 MPa | 7250 - 10200 psi | ASTM D638 |
Chang Chun Plastic PBT2000 Fire Retardant PBT Information provided by Dowell Trading Company Ltd. |
|||
Tensile Strength, Ultimate | 50.0 - 70.0 MPa | 7250 - 10200 psi | ASTM D638 |
Chang Chun Plastic PBT2100 Fire Retardant PBT Information provided by Dowell Trading Company Ltd. |